Physical Properties Metric English Comments
Melt Flow 0.15 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.15 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
SABIC F01552 High Density Polyethylene for Blown Film
Product Description: F01552 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh..
Melt Flow 0.15 - 0.30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.15 - 0.30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1283/L
NIZHNEKAMSKNEFTEKHIM PE 4148B (484H2) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 0.15 - 0.30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.15 - 0.30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1283/L
NIZHNEKAMSKNEFTEKHIM PE 6252J (526F2) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 0.15 - 0.30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.15 - 0.30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1283/L
NIZHNEKAMSKNEFTEKHIM PE 4252J (524F2) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 0.15 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.15 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Unipetrol PE HD LITEN® BB 29 HDPE
Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA
Melt Flow 0.15 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.15 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Unipetrol PE HD LITEN® BB 85 HDPE
Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA
Melt Flow 0.15 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.15 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Unipetrol PE HD LITEN® FB 29 HDPE
Made for tubular film applications.Information provided by Unipetrol RPA
Melt Flow 0.15 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.15 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Unipetrol PE HD LITEN® FB 85 HDPE
Made for tubular film applications.Information provided by Unipetrol RPA
Melt Flow 0.15 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.15 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Total MDPE HF 513 Medium Density Polyethylene, Blown Film
MDPE HF 513 is a medium density polyethylene produced by slurry loop low pressure process with hexene as co-monomer.MDPE HF 513 is a semi-high molecular weight polyethylene giving excellent mechanic..
Melt Flow 0.15 g/10 min

@Load 2.16 kg
0.15 g/10 min

@Load 4.76 lb
ASTM D 1238
Total HT 514 MDPE film
Finathene® HT 514 is a medium density polyethylene produced by the slurry loop low pressure polymerization process. Finathene® HT 514 can be used alone, blended or coextruded in a wide variety of ..
Melt Flow 0.15 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.15 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Total MDPE HT 514 Medium Density Polyethylene, Blown Film
MDPE HT 514 is a medium density polyethylene produced by slurry loop low pressure process with hexene as co-monomer.MDPE HT 514 is a semi-high molecular weight polyethylene giving excellent mechanic..
Melt Flow 0.15 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.15 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Unipetrol PE HD LITEN® VL 20 N HDPE
Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA
Melt Flow 0.15 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.15 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Unipetrol PE HD LITEN® ZB 20 HDPE
Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA