Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.33 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.33 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Unipetrol PE HD LITEN® VB 33 HDPE Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA |
|||
Melt Flow | 0.33 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.33 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM-D1238 |
Braskem GM9450F HDPE Blown Film Extrusion Polyethylene HDPE GM9450F is a high-density polyethylene developed for the high molecular weight film extrusion segment produced with bimodal technology. The film produced from this resin has high tenacity and e.. |
|||
Melt Flow | 0.33 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.33 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM D1238 |
Braskem Green PE SGM9450F Blow Film Extrusion and Cast Film Extrusion High Density Polyethylene Description: SGM9450F is a high-density polyethylene, developed for the high molecular weight film extrusion segment produced with bimodal technology. The film produced from this resin has high tena.. |
|||
Melt Flow | 0.33 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.33 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM-D1238 |
Braskem HB0454HR HDPE Blow Molding Polyethylene Copolymer HB0454HR is a high-density polyethylene copolymer resin with average molecular weight produced by the Unipol® process. A bottle made with HB0454HR shows excellent processability, color, and superfi.. |