Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 14 g/10 min @Load 5.00 kg, Temperature 190 °C |
14 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Eraclene® MM 84 High Density Polyethylene - Injection Molding Eraclene MM 84 is a high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.Eraclene MM 84 is characterized by high rigidity and good impact resistance. .. |
|||
Melt Flow | 14 g/10 min @Load 5.00 kg, Temperature 260 °C |
14 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D 1238 |
SABIC Innovative Plastics Cycoloy® EFX810ME PC Modified PC blend offering metallic / sparkle look with minimal flowline visibility.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 14 g/10 min @Load 5.00 kg, Temperature 260 °C |
14 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D 1238 |
SABIC Innovative Plastics Cycoloy® EFX810ME PC (Asia Pacific) Modified PC blend offering metallic look with minimal flowline visibility.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Melt Flow | 14 g/10 min @Load 3.80 kg, Temperature 230 °C |
14 g/10 min @Load 8.38 lb, Temperature 446 °F |
Cond I; ASTM D1238 |
Ravago Manufacturing Americas Hylac® HF143 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Melt Flow | 14 g/10 min @Load 1.20 kg, Temperature 300 °C |
14 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® ML7652 PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. Medium flow, excellent low temperature ductility.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 14 g/10 min @Load 10.0 kg, Temperature 220 °C |
14 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
SABIC Innovative Plastics Cycolac® BDT5510 ABS Automotive. High heat resistance, low gloss, color concentratable for interior applications. Natural only. |
|||
Melt Flow | 14 g/10 min @Load 3.80 kg, Temperature 190 °C |
14 g/10 min @Load 8.38 lb, Temperature 374 °F |
ASTM D1238 |
PolyOne Elastamax XL 1092-2 TPU-Based Thermoplastic Elastomer
(discontinued **) This is a general purpose thermoplastic elastomer based on modified TPU technology. Physical Form: Pellet. Standard Color: Natural.Information provided by M. A. Hanna. M. A. Hanna and Geon merged.. |
|||
Melt Flow | 14 g/10 min @Load 2.16 kg, Temperature 190 °C |
14 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Delrin® 500AL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 500AL is a medium viscosity acetal homopolymer, with an advanced system of lubrication for applications requiring low wear and/or coefficient of friction against steel, itself or other plas.. |
|||
Melt Flow | 14 - 42 g/10 min @Load 21.6 kg, Temperature 190 °C |
14 - 42 g/10 min @Load 47.6 lb, Temperature 374 °F |
|
Kazanorgsintez PE2NT 15-5 Linear Low Density Polyethylene Production Method: Gaseous-phase method. Application: Composition is intended to be processed into a stretch film.Information Provided by Kazanorgsintez |
|||
Melt Flow | 14 g/10 min @Load 10.0 kg, Temperature 220 °C |
14 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
LG Chemical 95HCTC SAN, High Transparency, Heat Resistance, Chemical Resistance Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Lighter, Cosmetic Container, ToothbrushCAS No. 9003-54-7Information provided by LG Chemical |
|||
Melt Flow | >= 14 g/10 min @Load 5.00 kg, Temperature 190 °C |
>= 14 g/10 min @Load 11.0 lb, Temperature 374 °F |
|
MTM Plastics Dipolen® SP Recycled PP Blend Dipolen® SP is a granulated polypropylene with other polyolefin blend for use in either extrusion or injection molding. It can be supplied unmodified or treated with additives according to custo.. |
|||
Melt Flow | 14 g/10 min @Load 1.20 kg, Temperature 280 °C |
14 g/10 min @Load 2.65 lb, Temperature 536 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Noryl V180HF PPE+HIPS (Europe-Africa-Middle East) NORYL V180HF is an unfilled, flame retardant material. It has been fully optimized w.r.t. flow and is halogen free according to VDE/DIN 472 part 815.This data was supplied by SABIC-IP for the Europe.. |
|||
Melt Flow | 14 g/10 min @Load 5.00 kg, Temperature 360 °C |
14 g/10 min @Load 11.0 lb, Temperature 680 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem 2312EPR PEI (Europe-Africa-Middle East) 30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Eu.. |
|||
Melt Flow | 14 g/10 min @Load 5.00 kg, Temperature 360 °C |
14 g/10 min @Load 11.0 lb, Temperature 680 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem DH1004F PEI High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Americas regi.. |
|||
Melt Flow | 14 g/10 min @Load 5.00 kg, Temperature 360 °C |
14 g/10 min @Load 11.0 lb, Temperature 680 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem DH1004F PEI (Europe-Africa-Middle East) High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Europe-Africa.. |
|||
Melt Flow | 14 g/10 min @Load 2.16 kg, Temperature 220 °C |
14 g/10 min @Load 4.76 lb, Temperature 428 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL N850 PPE+PS ECO-FLO(tm). ECO conforming, nonhalogenated flame retardant PPE+PS. High flow. Electrical and Business Equipment applications. |
|||
Melt Flow | 14 g/10 min @Load 2.16 kg, Temperature 220 °C |
14 g/10 min @Load 4.76 lb, Temperature 428 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL N850 PPE+PS (Asia Pacific) ECO-FLO(tm). ECO conforming, nonhalogenated flame retardant PPE+PS. High flow. Electrical and Business Equipment applications. |
|||
Melt Flow | 14 g/10 min @Load 1.20 kg, Temperature 300 °C |
14 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics XYLEX X8210 PC+POLYESTER PC+POLYESTER alloy. Unreinforced, transparent, impact modified for low temperature ductility |
|||
Melt Flow | 14 g/10 min @Load 2.16 kg, Temperature 140 °C |
14 g/10 min @Load 4.76 lb, Temperature 284 °F |
ASTM D1238 |
Lubrizol Estane® UB450 Thermoplastic Polyurethane Type: Estane® UB450 is a Shore A, polyester based, solvent-borne adhesive thermoplastic polyurethane (TPU).Uses: Solvent Coating.Available in AsiaInformation Provided by The Lubrizol Corporation |
|||
Melt Flow | 14 g/10 min @Load 5.00 kg, Temperature 230 °C |
14 g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
Borealis Borclean™ HC312BF Polypropylene Homopolymer for Capacitor Film Borclean HC312BF is a homopolymer film resin developed for use in the manufacture of the highest quality films for dielectric applications. Borclean HC312BF does not contain slip, antiblock, antist.. |
|||
Melt Flow | 14 g/10 min @Load 2.16 kg, Temperature 190 °C |
14 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Unipetrol PE HD LITEN® FB 10 HDPE Made for tubular film applications.Information provided by Unipetrol RPA |
|||
Melt Flow | 14 g/10 min @Load 2.16 kg, Temperature 260 °C |
14 g/10 min @Load 4.76 lb, Temperature 500 °F |
ISO 1133 |
Polyplastics TOPAS® 6013 Cyclic Olefin Copolymer (COC) (Asia/Pacific Grade) Due to its high transparency, low levels of eluates, superior chemical resistance, and high heat deflection temperature, this grade is suitable for products such as pharmaceutical packaging and diag.. |
|||
Melt Flow | 14 g/10 min @Load 3.80 kg, Temperature 230 °C |
14 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Chi Mei Kibisan® PN-117 SAN Injection Molding |
|||
Melt Flow | 14 g/10 min @Load 2.16 kg, Temperature 190 °C |
14 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Delrin® 500TL NC010 Acetal (POM)
(Unverified Data**) Teflon® Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500TL is a medium viscosity acetal homopolymer resin containing 1.5% Teflon PTFE Micropowder. It is desi.. |
|||
Melt Flow | 14 g/10 min @Load 2.16 kg, Temperature 190 °C |
14 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Delrin® 511DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium Viscosity Acetal Homopolymer Delrin 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage less s.. |
|||
Melt Flow | 14 g/10 min @Load 2.16 kg, Temperature 190 °C |
14 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Delrin® FG500TL NC010 Acetal (POM)
(Unverified Data**) Teflon® Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact ApplicationsDelrin FG500TL medium viscosity acetal homopolymer resin containing 1.5%.. |
|||
Melt Flow | 14 g/10 min @Load 2.16 kg, Temperature 190 °C |
14 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Delrin® FG511DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for mo.. |
|||
Melt Flow | 14 g/10 min @Load 3.80 kg, Temperature 230 °C |
14 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Diamond Polymers ABS 2501 Injection Molding Grade, Medium Impact, High Flow Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 14 g/10 min @Load 3.80 kg, Temperature 230 °C |
14 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ABS 2512 Description: Injection Molding Grade, Medium Impact, High FlowInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 14 g/10 min @Load 2.16 kg, Temperature 190 °C |
14 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Delrin® 500PE BK602 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE BK602 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi.. |