Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 24 g/10 min @Load 2.16 kg, Temperature 190 °C |
24 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
PolyOne Versaflex™ OM 9-802CL Thermoplastic Elastomer (TPE) Versaflex™ OM 9-802CL is a clear, soft touch TPE designed to bond to the following thermoplastics: PC, ABS, PC/ABS and copolyester. New Product. Commercial specifications have not been established... |
|||
Melt Flow | 24 g/10 min @Load 10.0 kg, Temperature 220 °C |
24 g/10 min @Load 22.0 lb, Temperature 428 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Cycolac® GPM5500 ABS (Europe-Africa-Middle East) CYCOLAC GPM5500 is a multi purpose injection moulding grade, providing a favourable balance of engineering properties. CYCOLAC GPM5500 has a wide processing window. It is recommended for application.. |
|||
Melt Flow | 24 g/10 min @Load 10.0 kg, Temperature 220 °C |
24 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
SABIC Innovative Plastics Cycolac® GPM5500F ABS (Europe-Africa-Middle East) CYCOLAC GPM5500F is a multi purpose injection moulding grade, providing a favourable balance of engineering properties and is FDA and European Directive 2002/72/EC
(FCEU) compliant for food contac.. |
|||
Melt Flow | 24 g/10 min @Load 10.0 kg, Temperature 220 °C |
24 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
SABIC Innovative Plastics Cycolac® GPM5500S ABS (Europe-Africa-Middle East) CYCOLAC GPM5500S is a multi purpose injection moulding grade, equal to GPM5500 but equiped with anti static agents, providing a favourable balance of engineering properties. CYCOLAC GPM5500S has a w.. |
|||
Melt Flow | 24 g/10 min @Load 10.0 kg, Temperature 220 °C |
24 g/10 min @Load 22.0 lb, Temperature 428 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Cycolac® GPM5500S ABS (Europe-Africa-Middle East) CYCOLAC GPM5500S is a multi purpose injection moulding grade, equal to GPM5500 but equiped with anti static agents, providing a favourable balance of engineering properties. CYCOLAC GPM5500S has a w.. |
|||
Melt Flow | 24 g/10 min @Load 10.0 kg, Temperature 220 °C |
24 g/10 min @Load 22.0 lb, Temperature 428 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Cycolac® GPM5500U ABS (Europe-Africa-Middle East) CYCOLAC GPM5500U is a UV stabilized multi purpose injection moulding grade, providing a favourable balance of engineering properties. CYCOLAC GPM5500U has a wide processing window. It is recommended.. |
|||
Melt Flow | 24 g/10 min @Load 5.00 kg, Temperature 260 °C |
24 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D 1238 |
SABIC Innovative Plastics Cycoloy® C1204HF PC+ABS (Europe-Africa-Middle East) High heat PC/ABS blend offering good flow and excellent impact. Food compliant according to FDA and European directive 2002/72/EC. Available in limited colors. Effective January 15th, 2008 this gra.. |
|||
Melt Flow | 24 g/10 min @Load 5.00 kg, Temperature 300 °C |
24 g/10 min @Load 11.0 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Cycoloy® CE1810 PC+ABS (Asia Pacific) PC/ABS with high stiffness and low CTE.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Melt Flow | 24 g/10 min @Load 5.00 kg, Temperature 300 °C |
24 g/10 min @Load 11.0 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Cycoloy® CE1810 PC+ABS (Europe-Africa-Middle East) PC/ABS with high stiffness and low CTE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Melt Flow | 24 - 36 g/10 min @Load 21.6 kg, Temperature 190 °C |
24 - 36 g/10 min @Load 47.6 lb, Temperature 374 °F |
Flow@21.6kg/Flow@2.16kg ratio < 30; ASTM D1283 |
NIZHNEKAMSKNEFTEKHIM PE 4115N (16401) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 24 - 36 g/10 min @Load 21.6 kg, Temperature 190 °C |
24 - 36 g/10 min @Load 47.6 lb, Temperature 374 °F |
Flow@21.6kg/Flow@2.16kg ratio < 30; ASTM D1283 |
NIZHNEKAMSKNEFTEKHIM PE 4116N (16401) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 24 - 36 g/10 min @Load 21.6 kg, Temperature 190 °C |
24 - 36 g/10 min @Load 47.6 lb, Temperature 374 °F |
Flow@21.6kg/Flow@2.16kg ratio < 30; ASTM D1283 |
NIZHNEKAMSKNEFTEKHIM PE 4117N (18401) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 24 - 36 g/10 min @Load 21.6 kg, Temperature 190 °C |
24 - 36 g/10 min @Load 47.6 lb, Temperature 374 °F |
Flow@21.6kg/Flow@2.16kg ratio < 30; ASTM D1283 |
NIZHNEKAMSKNEFTEKHIM PE 5118N (18601) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 24 g/10 min @Load 5.00 kg, Temperature 300 °C |
24 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HPS7 PC (Europe-Africa-Middle East) Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. .. |
|||
Melt Flow | 24 g/10 min @Load 5.00 kg, Temperature 200 °C |
24 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
PolyOne Dynaflex™ G2711-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2711-1000-00 is an easy process compound designed for injection molding and extrusion applications that require FDA compliance. - Excellent Colorability - Good Ozone and UV Stability - O.. |
|||
Melt Flow | 24 g/10 min @Load 1.20 kg, Temperature 300 °C |
24 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® FXE173R PC This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 24 g/10 min @Load 5.00 kg, Temperature 300 °C |
24 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HPS7 PC Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. .. |
|||
Melt Flow | 24 g/10 min @Load 5.00 kg, Temperature 300 °C |
24 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HPS7 PC (Asia Pacific) Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. .. |
|||
Melt Flow | 24 g/10 min @Load 5.00 kg, Temperature 230 °C |
24 g/10 min @Load 11.0 lb, Temperature 446 °F |
ASTM D1238 |
Solvay Specialty Polymers Solef® 21508 PVDF Copolymer
(discontinued **) Key features of this grade: High Elongation, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® P.. |
|||
Melt Flow | 24 g/10 min @Load 5.00 kg, Temperature 230 °C |
24 g/10 min @Load 11.0 lb, Temperature 446 °F |
ASTM D1238 |
Solvay Specialty Polymers Solef® 3208/0150 Anti-friction PVDF Compound
(discontinued **) Key features of this grade: Anti-friction, Formulated. Recommended processing is injection. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crysta.. |
|||
Melt Flow | 24 g/10 min @Load 2.16 kg, Temperature 265 °C |
24 g/10 min @Load 4.76 lb, Temperature 509 °F |
ASTM D1238 |
Global XNY-1424 Easy Flow Polycarbonate/Polyester Alloy Information provided by Global Polymers Corporation. |
|||
Melt Flow | >= 24 g/10 min @Load 5.00 kg, Temperature 190 °C |
>= 24 g/10 min @Load 11.0 lb, Temperature 374 °F |
|
MTM Plastics Dipolen® PP Recycled PP Dipolen® PP is a granulated polypropylene for use in either extrusion or injection molding. It can be supplied unmodified or treated with additives according to customer specifications. DipolenÂ.. |
|||
Melt Flow | 24 g/10 min @Load 6.60 kg, Temperature 337 °C |
24 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D 1238 |
SABIC Innovative Plastics Ultem HATX200 PEI+PCE (Asia Pacific) High flow Polyetherimide blend. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compli.. |
|||
Melt Flow | 24 g/10 min @Load 6.60 kg, Temperature 337 °C |
24 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D 1238 |
SABIC Innovative Plastics Ultem HATX200 PEI+PCE (Europe-Africa-Middle East) High flow Polyetherimide blend. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compli.. |
|||
Melt Flow | 24 g/10 min @Load 3.80 kg, Temperature 200 °C |
24 g/10 min @Load 8.38 lb, Temperature 392 °F |
ASTM D 1238 |
SABIC Innovative Plastics Noryl GTX GTX9200 PPE+PS+PA66 High Flow GTX for Automotive applicationsThis data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 24 g/10 min @Load 2.16 kg, Temperature 230 °C |
24 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis MG302Al Polypropylene Compound, Mineral Filled MG302AI is a 30% mineral filled polypropylene compound intended for injection and back injection molding. This material has an excellent balance between impact strength and stiffness and high melt .. |
|||
Melt Flow | 24 g/10 min @Load 21.6 kg, Temperature 190 °C |
24 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM-D1238 |
Braskem BS002HS HDPE Blow Molding Polyethylene Copolymer Resin BS002HS is a high-density polyethylene, bimodal copolymer. It presents good rigidity, good impact resistance, and good reproducibility of the weight of the bottles. It also has excellent envir.. |
|||
Melt Flow | 24 g/10 min @Load 5.00 kg, Temperature 230 °C |
24 g/10 min @Load 11.0 lb, Temperature 446 °F |
ASTM D1238 |
Solvay Specialty Polymers Solef® 1008 PVDF Homopolymer
(discontinued **) Key features of this grade: Low Viscosity, All Purpose, Injection, Virgin. Recommended processing is injection. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF .. |
|||
Melt Flow | 24 g/10 min @Load 5.00 kg, Temperature 230 °C |
24 g/10 min @Load 11.0 lb, Temperature 446 °F |
ASTM D1238 |
Solvay Specialty Polymers Solef® 11008 PVDF Copolymer
(discontinued **) Key features of this grade: Low Viscosity, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVD.. |
|||
Melt Flow | 24 g/10 min @Load 5.00 kg, Temperature 300 °C |
24 g/10 min @Load 11.0 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Cycoloy® CE1810 PC+ABS PC/ABS with high stiffness and low CTE.This data was supplied by SABIC-IP for the Americas region. |