Polymer Property : Oxygen Transmission = 0.0200 cc-mm/m²-24hr-atm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxygen Transmission 0.0200 cc-mm/m²-24hr-atm
0.0508 cc-mil/100 in²-24hr-atm
20°C- 65% RH; based on 20 µm layer
Noltex Soarnol® BS3803 Ethylene Vinyl Alcohol Copolymer
Modified ET3803; New Stretchable EVOH. Ethylene content 38 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of nylon, therefore, Soarnol allows ..
Oxygen Transmission 0.0200 cc-mm/m²-24hr-atm
0.0508 cc-mil/100 in²-24hr-atm
metallized barrier; 6 cc/100in²-24hr-atm unmetallized barrier; Tested per ASTM D1434 at 77°F, 75% RH.
DuPont Teijin Films Mylar® 813 Polyester Packaging Film, 48 Gauge
Data provided by DuPont Packaging Polymers.Melinex® 813 is a polyester film, pretreated on one side to provide excellent adhesion to a wide range of both solvent- and water-based inks. Melinex® 8..
Oxygen Transmission 0.0200 cc-mm/m²-24hr-atm
0.0508 cc-mil/100 in²-24hr-atm
metallized barrier; 6 cc/100in²-24hr-atm unmetallized barrier; Tested per ASTM D1434 at 77°F, 75% RH.
DuPont Teijin Films Mylar® 800 Polyester Packaging Film, 48 Gauge
Data provided by DuPont Packaging Polymers.Melinex® 800 is a clear, non-pretreated base film with high gloss, low haze and excellent processability. Melinex® 800 is available in 48 gauge. Meline..