Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 0.200 cc-mm/m²-24hr-atm | 0.508 cc-mil/100 in²-24hr-atm | or 9 cc/m²-24hr-atm for the film. ASTM D3985 |
DuPont Teijin Films Mylar® M34 Polyester Film, 75 Gauge (20 µm), PVDC Coated Data provided by DuPont Packaging Polymers.A transparent polyester packaging film, solvent coated on one side with a PVDC copolymer. The coating is heat sealable, and is an excellent moisture and o.. |
|||
Oxygen Transmission | 0.200 cc-mm/m²-24hr-atm | 0.508 cc-mil/100 in²-24hr-atm | or 8 cc/m²-24hr-atm for the film. ASTM D3985 |
DuPont Teijin Films Mylar® M30 Polyester Film, 75 Gauge (21 µm), PVDC Coated
(discontinued **) Data provided by DuPont Packaging Polymers.A transparent polyester packaging film, solvent coated on both sides with a PVDC copolymer. The coating is heat sealable, and is an excellent moisture and.. |
|||
Oxygen Transmission | 0.200 cc-mm/m²-24hr-atm | 0.508 cc-mil/100 in²-24hr-atm | or 8 cc/m²-24hr-atm for the film. ASTM D3985 |
DuPont Teijin Films Mylar® M30 Polyester Film, 100 Gauge (25 µm), PVDC Coated
(discontinued **) Data provided by DuPont Packaging Polymers.A transparent polyester packaging film, solvent coated on both sides with a PVDC copolymer. The coating is heat sealable, and is an excellent moisture and.. |