Physical Properties Metric English Comments
Oxygen Transmission 0.472 cc-mm/m²-24hr-atm
1.20 cc-mil/100 in²-24hr-atm
10% RH; ASTM D3985
Dow SARAN WRAP™ 18 Plastic Film
SARAN WRAP™ 18 Plastic Film is a clear biaxially oriented monolayer barrier film, designed for chub packaging machines and laminations. It is available in 100 gauge, as single or double would roll..
Oxygen Transmission 0.472 cc-mm/m²-24hr-atm
1.20 cc-mil/100 in²-24hr-atm
10% RH; ASTM D3985
Dow Saran® 18L Clear Plastic Barrier Film
Saran™ 18L is a clear biaxially oriented monolayer barrier film, preshrunk for lamination applications. It is available in 75 gauge, as single or double wound rolls.Information provided by Dow
Oxygen Transmission 0.472 cc-mm/m²-24hr-atm
1.20 cc-mil/100 in²-24hr-atm
10% RH; ASTM D3985
Dow SARAN WRAP™ 3 Plastic Film
SARAN WRAP™ 3 Plastic Film is a clear biaxially oriented monolayer barrier film, designed for tight wrap and heat sealing applications. It is available in 50 gauge, as single or double would rolls..