Polymer Property : Oxygen Transmission = 0.508 cc-mil/100 in²-24hr-atm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxygen Transmission 0.200 cc-mm/m²-24hr-atm
0.508 cc-mil/100 in²-24hr-atm
or 9 cc/m²-24hr-atm for the film. ASTM D3985
DuPont Teijin Films Mylar® M34 Polyester Film, 75 Gauge (20 µm), PVDC Coated
Data provided by DuPont Packaging Polymers.A transparent polyester packaging film, solvent coated on one side with a PVDC copolymer. The coating is heat sealable, and is an excellent moisture and o..
Oxygen Transmission 0.200 cc-mm/m²-24hr-atm
0.508 cc-mil/100 in²-24hr-atm
or 8 cc/m²-24hr-atm for the film. ASTM D3985
DuPont Teijin Films Mylar® M30 Polyester Film, 75 Gauge (21 µm), PVDC Coated  (discontinued **)
Data provided by DuPont Packaging Polymers.A transparent polyester packaging film, solvent coated on both sides with a PVDC copolymer. The coating is heat sealable, and is an excellent moisture and..
Oxygen Transmission 0.200 cc-mm/m²-24hr-atm
0.508 cc-mil/100 in²-24hr-atm
or 8 cc/m²-24hr-atm for the film. ASTM D3985
DuPont Teijin Films Mylar® M30 Polyester Film, 100 Gauge (25 µm), PVDC Coated  (discontinued **)
Data provided by DuPont Packaging Polymers.A transparent polyester packaging film, solvent coated on both sides with a PVDC copolymer. The coating is heat sealable, and is an excellent moisture and..