Polymer Property : Oxygen Transmission = 0.600 cc-mm/m²-24hr-atm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxygen Transmission 0.00400 - 0.600 cc-mm/m²-24hr-atm
0.0102 - 1.52 cc-mil/100 in²-24hr-atm
Average value: 0.0397 cc-mm/m²-24hr-atm Grade Count:28
Overview of materials for Ethylene Vinyl Alcohol (EVOH)
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Alcohol". Each property range of values reported is minimum and maximum values of appropr..