Polymer Property : Oxygen Transmission = 32.0 cc-mm/m²-24hr-atm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxygen Transmission 32.0 cc-mm/m²-24hr-atm
81.3 cc-mil/100 in²-24hr-atm
ASTM D3985
Eastman Tritan FX100 Copolyester
Eastman Tritan FX100 is an amorphous copolyester that combines clarity and toughness with heat and chemical resistance. Films manufactured from this new-generation copolyester can be thermoformed w..
Oxygen Transmission 32.0 cc-mm/m²-24hr-atm
81.3 cc-mil/100 in²-24hr-atm
ASTM D3985
Eastman Tritan MP100 Copolyester
Eastman Tritan MP100 is an amorphous copolyester that combines excellent clarity and toughness with outstanding heat and chemical resistance. Film and sheet manufactured from this new-generation co..
Oxygen Transmission 32.0 cc-mm/m²-24hr-atm
81.3 cc-mil/100 in²-24hr-atm
36% Cl content Tyrin resin w/ Ba-Cd stabilizer, Epoxidized soybean oil, phosphite chelator, and lubricant.
Dow Tyrin® 3615P Chlorinated Polyethylene Elastomer
36% Chlorine. Tyrin® chlorinated polyethylene thermoplastic resins offer the compounding and fabrication industries end product properties in a range of hardnesses, and behave much like flexible P..
Oxygen Transmission 32.0 cc-mm/m²-24hr-atm
81.3 cc-mil/100 in²-24hr-atm
36% Cl content Tyrin resin w/ Ba-Cd stabilizer, Epoxidized soybean oil, phosphite chelator, and lubricant.
Dow Tyrin® 3611P Chlorinated Polyethylene Elastomer
36% Chlorine. Tyrin® chlorinated polyethylene thermoplastic resins offer the compounding and fabrication industries end product properties in a range of hardnesses, and behave much like flexible P..
Oxygen Transmission 32.0 cc-mm/m²-24hr-atm
81.3 cc-mil/100 in²-24hr-atm
36% Cl content Tyrin resin w/ Ba-Cd stabilizer, Epoxidized soybean oil, phosphite chelator, and lubricant.
Dow Tyrin® 3623A Chlorinated Polyethylene Elastomer
36% Chlorine. Tyrin® chlorinated polyethylene thermoplastic resins offer the compounding and fabrication industries end product properties in a range of hardnesses, and behave much like flexible P..
Oxygen Transmission 32.0 cc-mm/m²-24hr-atm
81.3 cc-mil/100 in²-24hr-atm
36% Cl content Tyrin resin w/ Ba-Cd stabilizer, Epoxidized soybean oil, phosphite chelator, and lubricant.
Dow Tyrin® CM2136P Chlorinated Polyethylene Elastomer
36% Chlorine. Tyrin® chlorinated polyethylene thermoplastic resins offer the compounding and fabrication industries end product properties in a range of hardnesses, and behave much like flexible P..