Physical Properties | Metric | English | Comments |
---|---|---|---|
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | ASTM D1693 |
NIZHNEKAMSKNEFTEKHIM PE 6948C (486H3) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | Condition A (100% Igepal), F<sub>50</sub>; ASTM D1693 |
Formosa Plastics Formolene® L43840U Rotational Molding LLDPE
(discontinued **) Butene CopolymerApplications: Toys and other non-tank rotational molding applications.Formolene L43840U is a Butene Copolymer of linear low density polyethylene for toys and other non-tank rotationa.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | (100% Igepal), F<sub>50</sub>; ASTM D1693 |
Formosa Plastics Formolene® L63565 Rotational Molding LLDPE
(discontinued **) Hexene CopolymerApplications: Toys, medium tanks, material handling equipment and flat surface rotational molding applications.Meets all requirements of the U.S. Food and Drug Administration as spec.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour @Temperature 50.0 °C |
>= 1000 hour @Temperature 122 °F |
Condition A; ASTM D 1693 |
Chevron Phillips Marlex® CL-200YJN (Natural) Rotational molding crosslinkable high density polyethylene
(disc Benefits: crosslinks during molding - has outstanding melt strength at 204°C, is formulated to provide maximum UV protection for long-term outdoor weathering, contains an internal mold release, exc.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | F0, ASTM D1693 |
NOVA Chemicals Sclair® 96A HDPE Extrusion Resin
(discontinued **) Features: Excellent processability, excellent stretchability, superior strength, gel free.Applications: Oriented tapes for industrial woven bags and tarpaulins, monoaxial oriented films.Data provide.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | ASTM D1693 |
ExxonMobil HD 9856BA Blow Molding Resin
(discontinued **) HD 9856BA is a HDPE blow molding resin designed for high performance packaging applications. Containers made from HD 9856BA exhibit a unique combination of stiffness and environmental stress cracki.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | F50, Condition A; ASTM D1693 |
ExxonMobil Escorene® LD-409 EVA for Low Voltage Insulation
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A crosslinkable, 9.9% vinyl acetate copolymer designed for electrical applications.Applications: Designed to be blended with a suitable masterbatch .. |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | 10% Igepal®, F<sub>50</sub>; ASTM D1693 |
LyondellBasell Petrothene® GA808093 Linear Low Density Polyethylene ApplicationsPETROTHENE GA 808-093 is a broad molecular weight, linear low density polyethylene resin designed for use as a wire and cable insulation. An antioxidant package is added to ensure therm.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | Condition A - 10% Igepal®; ASTM D1693 |
LyondellBasell Petrothene® KR92828 High Density Polyethylene ApplicationsPETROTHENE KR 92828 is a high molecular weight, high density polyethylene-based compound designed for use in jacketing, conduit or wire insulation. KR 92828 contains a carbon black cont.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | F<sub>50</sub>; ASTM D1693 |
LyondellBasell Petrothene® LP500200 High Density Polyethylene (Sheet & Profile Grade) ApplicationsThe PETROTHENE LP 5002 series of polyethylene resins exhibits excellent environmental stress crack resistance.Regulatory StatusThe LP 5002 base resin meets the requirements of Food and D.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | F<sub>50</sub>; ASTM D1693 |
LyondellBasell Petrothene® LP500210 High Density Polyethylene (Sheet & Profile Grade) ApplicationsThe PETROTHENE LP 5002 series of polyethylene resins exhibits excellent environmental stress crack resistance.Regulatory StatusThe LP 5002 base resin meets the requirements of Food and D.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | M F50; ASTM D1693 |
Micropol Microlink XL28 Crosslinkable Polyethylene Provides a finished molding of improved properties with the use of conventional rotational molding equipment. Properties include enhanced toughness (particularly low temp impact), ESCR, chemical, a.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | M F50; ASTM D1693 |
Micropol Microlink XL28/FR Black Crosslinkable Polyethylene Flame retardant. Provides a finished molding of improved properties with the use of conventional rotational molding equipment. Properties include enhanced toughness (particularly low temp impact),.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | Condition B, F50; ASTM D1693 |
IRPC Polimaxx Polene AM3245 PC High Density Polyethylene CHARACTERISTICS:GOOD EXTRUDABILITYHIGH PRESSURE PIPE FOLLOW-UP MINIMUM REQUIRED STRENGTH OF 10.0 MPa (DESIGN STRESS OF 8.0 MPa) CLASSIFICATION PE100BLACK COLOR COMPOUNDAPPLICATIONS: PIPE EXTRUSIONSU.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | Condition B, F50; ASTM D1693 |
IRPC Polimaxx Polene GA3245 High Density Polyethylene CHARACTERISTICS: HIGH TOUGHNESS, GOOD EXTRUDABILITY, EXCELLENT IMPACT STRENGTHAPPLICATIONS: BLOW FILM EXTRUSION FOR CARRIER BAGS, GROCERY BAGS, SHOPPING BAGS, INDUSTRIAL BAGS, LINER BAGS |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | Condition B, F50; ASTM D1693 |
IRPC Polimaxx Polene GA3750 High Density Polyethylene CHARACTERISTICS: GOOD EXTRUDABILITY, HIGH IMPACT STRENGTHAPPLICATIONS: BLOW FILM EXTRUSION FOR SHOPPING BAGS, GROCERY BAGS |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | F<sub>50</sub>; ASTM D1693 |
LyondellBasell Petrothene® LP5100 High Density Polyethylene ApplicationsPETROTHENE LP 5100 is especially designed for large-part blow molding of durable goods and deep-draw sheet extrusion/thermoforming applications. LP 5100 exhibits excellent impact resist.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour @Thickness 3.00 mm, Temperature 50.0 °C |
>= 1000 hour @Thickness 0.118 in, Temperature 122 °F |
Condition A, Compression Molded, 10% Igepal; ASTM D1693 |
Solvay Specialty Polymers Cogegum® AFR/720-UV Polyolefin Cogegum® HFFR -Halogen Free Fire Retardant compound. Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties with.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour @Thickness 3.00 mm, Temperature 50.0 °C |
>= 1000 hour @Thickness 0.118 in, Temperature 122 °F |
Condition A, Compression Molded, 10% Igepal; ASTM D1693 |
Solvay Specialty Polymers Cogegum® GFR/350 Polyolefin Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound. Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a pol.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour @Temperature 50.0 °C |
>= 1000 hour @Temperature 122 °F |
F50, 25% Igepal; ASTM D1639 |
SCG Chemicals EL-Leneâ„¢ L2009F Linear Low Density Polyethylene Film Key Characteristics:High productivityGood optical propertiesCan be blended with HDPE and LDPE to improve tear resistance and seal strengthContains 1000 ppm slip agent and 700 ppm antiblocking agentR.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour @Temperature 50.0 °C |
>= 1000 hour @Temperature 122 °F |
F50, 25% Igepal; ASTM D1639 |
SCG Chemicals EL-Leneâ„¢ L2009FA Linear Low Density Polyethylene Film Key Characteristics:High productivityGood optical propertiesCan be blended with HDPE and LDPE to improve tear resistance and seal strengthContains no slip agent and antiblocking agentRecommended App.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour @Temperature 50.0 °C |
>= 1000 hour @Temperature 122 °F |
F50, 25% Igepal; ASTM D1639 |
SCG Chemicals EL-Leneâ„¢ L2020F Linear Low Density Polyethylene Film Key Characteristics:High output and elongationContains 1800 ppm slip agent and 1400 ppm antiblocking agentRecommended Applications:General purpose bag, cast film, small bag, merchandise bag, printed.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | No failures; ASTM D1693 cond. C 100% lgepal |
Total HP 401N Natural HDPE, pipe Applications: Potable water, gas distribution, industrial and mining, sewer and sewer relining, gas and oil gathering, fiber optic innerduct, general pipe reliningInformation provided provided by T.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour @Temperature 50.0 °C |
>= 1000 hour @Temperature 122 °F |
Condition B; ASTM D 1693 |
Chevron Phillips Marlex® HXB TR-512 Extra high molecular weight polyethylene Benefits: outstanding impact and creep resistance, excellent ESCR, excellent chemical resistanceCharacteristics: ESCR > 700 at Condition A, at 50°C; ASTM D 1693Applications: 55-gallon drums, indust.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour @Temperature >=50.0 °C |
>= 1000 hour @Temperature >=122 °F |
Igepal (no failures); ASTM F1248 |
CPC - Vycom HITEC® Pipe Grade HDPE High Density Polyethylene Hitec pipe grade HDPE is a special formulation that has high impact strength, and environmental stress crack resistance. Hitec Pipe grade meets Federal specification L-P 390C, ASTM D1248 Type III we.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour @Temperature 50.0 - 50.0 °C |
>= 1000 hour @Temperature 122 - 122 °F |
Average value: 1000 hour Grade Count:5 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Film Grade". Each property range of values reported is minimum .. |
|||
Environmental Stress Crack Resistance | >= 1000 hour @Temperature 50.0 °C |
>= 1000 hour @Temperature 122 °F |
Igepal 100%; F20; IEC 60811-4-1/B |
Borealis LE6022 Polyethylene Modified Jacketing Compound LE6022 is a black low density copolymer modified polyethylene compound. It is characterized by excellent crack resistance and mechanical properties and low temperature performance in combination wit.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour @Thickness 3.00 mm, Temperature 50.0 °C |
>= 1000 hour @Thickness 0.118 in, Temperature 122 °F |
Condition A, Compression Molded, 10% Igepal; ASTM D1693 |
Solvay Specialty Polymers Cogegum® AFR/960 Polyolefin Cogegum® HFFR -Halogen Free Fire Retardant compound. Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties withou.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | ASTM D1693 cond. C 100% lgepal |
Total Finathene® CD 481 HDPE conduit
(discontinued **) Applications: Wire and cable conduit, fiber optic innerductInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines. |
|||
Environmental Stress Crack Resistance | >= 1000 hour @Temperature 50.0 - 50.0 °C |
>= 1000 hour @Temperature 122 - 122 °F |
Average value: 1000 hour Grade Count:3 |
Overview of materials for High Density Polyethylene (HDPE), Crosslinkable This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Crosslinkable". Each property range of values reported is minimum and .. |