Physical Properties | Metric | English | Comments |
---|---|---|---|
Environmental Stress Crack Resistance | 35 hour | 35 hour | Condition B, F<sub>50</sub> |
Chevron Phillips Marlex® HHM 5502-02 LW High Density Ethylene Hexene Copolymer
(discontinued **) High Density Ethylene Hexene Copolymer with Synthetic AntistatCustomer Benefits: The resin allows the blow molder to reduce inventory of resin types, because it can be used to package bleach and mos.. |
|||
Environmental Stress Crack Resistance | 35 hour | 35 hour | Condition B; ASTM D1693 |
I. Stern IS-35955 High Density Polyethylene, Blow Molding Grade Features:IS-35955 is designed for applications requiring excellent stiffness and stress crack resistance properties.Meets all requirements of the U. S. Food and Drug Administration as specified in 2.. |
|||
Environmental Stress Crack Resistance | 35 hour | 35 hour | ASTM D1693 cond. B 10% lgepal |
Total 5502 BZ HDPE injection blow molding Applications: Cosmetics and toiletries, pharmaceuticals, specialty containers, food packagingInformation provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atof.. |
|||
Environmental Stress Crack Resistance | 35 hour | 35 hour | Condition B, F<sub>50</sub>; ASTM D1693 |
Formosa Plastics Formolene® HB5502A Blow Molding HDPE High Density Polyethylene Hexene Copolymer for Blow Molding – With Antistat Formolene® HB5502A is designed for applications requiring excellent stiffness and stress crack resistance properties. It.. |
|||
Environmental Stress Crack Resistance | 35 hour | 35 hour | Condition B, F<sub>50</sub>; ASTM D1693 |
Formosa Plastics Formolene® HB5502S1 Sheet and Thermoforming HDPE High Density Polyethylene Hexene CopolymerApplications: Molded or formed industrial housings and parts, tanks, shrouds.Formolene HB5502S1 HDPE resin is designed for applications requiring excellent .. |
|||
Environmental Stress Crack Resistance | 35 hour | 35 hour | Condition B, F<sub>50</sub>; ASTM D1693 |
Formosa Plastics Formolene® HB5502Z Blow Molding HDPE Hexene CopolymerApplications: Injection blow molded pharmaceutical packagingFormolene HB5502Z eliminates the need for including a mold release agent at each machine, by incorporating zinc stearate w.. |
|||
Environmental Stress Crack Resistance | 35 hour | 35 hour | Condition B, F<sub>50</sub>; ASTM D1693 |
Formosa Plastics Formolene® HB5502B Blow Molding HDPE Hexene CopolymerApplications: Injection blow molded pharmaceutical packagingFormolene HB5502B is designed for applications requiring excellent stiffness and stress crack resistance properties. It ma.. |
|||
Environmental Stress Crack Resistance | 35 hour | 35 hour | Condition B, F<sub>50</sub> |
Chevron Phillips Marlex® HHM 5502 BN High Density Ethylene Hexene-1 Copolymer High Density Ethylene Hexene-1 CopolymerCustomer Benefits: This resin allows the blow molder to reduce inventory of resin types, because it can be used to package a wide range of products. Has exce.. |
|||
Environmental Stress Crack Resistance | 35 hour | 35 hour | Condition B, F<sub>50</sub>; ASTM D1693 |
Formosa Plastics Formolene® HB5502B2 Blow Molding HDPE Hexene CopolymerApplications: Pharmaceutical Packaging; Personal Care Products;
Bleach and Detergents Industrial; and Chemicals & PartsFormolene® HB5502B2 is designed for applications requiring ex.. |