Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 11000 - 13000 cP | 11000 - 13000 cP | |
Guarniflon TENFIL TF 200 Polytetrafluoroethylene Thread Sealant TENFIL TF200 is a PTFE-based thread sealant in water dispersion, which increases the tightness of the threaded parts and prevents leakage of water. The product is intended for the assembly of fitti.. |
|||
Brookfield Viscosity | 11000 - 13000 cP | 11000 - 13000 cP | |
Guarniflon TENFIL TF 400 Polytetrafluoroethylene Thread Sealant TENFIL TF400 is a PTFE-based thread sealant in water dispersion, which increases the tightness of the threaded parts and prevents leakage of water. The product is intended for the assembly of fitti.. |
|||
Brookfield Viscosity | 11000 cP | 11000 cP | Base, RVF #7 spindle, 20 rpm |
3M Scotch-Weld™ DP405 LH Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP405 LH is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive which has a 5 minute work life and accelerated cure. It exhibits excellent shear and peel.. |
|||
Brookfield Viscosity | 11000 - 15000 cP | 11000 - 15000 cP | Base, RVF #7 spindle, 20 rpm |
3M Scotch-Weld™ 2216 B/A Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel.. |
|||
Brookfield Viscosity | 11000 cP | 11000 cP | Base, RVF #7 spindle, 20 rpm |
3M Scotch-Weld™ DP405 Black Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP405 LH is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive which has a 5 minute work life and accelerated cure. It exhibits excellent shear and peel.. |
|||
Brookfield Viscosity | 11000 cP @Temperature 25.0 °C |
11000 cP @Temperature 77.0 °F |
Mixed |
Loctite® Durabond® M-121HP Epoxy Adhesive Medical Grade BondersLoctite offers the most comprehensive line of adhesives and sealants available to the medical device industry. These USP class VI and/or ISO-10993 compliant products are designe.. |