Physical Properties | Metric | English | Comments |
---|---|---|---|
Surface Tension | 33 dynes/cm | 33 dynes/cm | |
Solvay Specialty Polymers Diofan® A602 Polyvinylidene Chloride (PVDC)
(discontinued **) DIOFAN® A602 is a water based dispersion of a polyvinylidene chloride copolymer. It is free of solvent traces, alkylphenol ethoxylates or any other toxic substances. It features strong barrier prop.. |
|||
Surface Tension | 33 - 43 dynes/cm | 33 - 43 dynes/cm | |
Dow Latex XZ 92199.00 Experimental Latex Description: XZ 92199.00 Experimental latex is an aqueous dispersion of a modified carboxylated styrene butadiene copolymer. It has been developed for use as an adhesive latex for secondary backed t.. |
|||
Surface Tension | 33 dynes/cm | 33 dynes/cm | Ring Method |
Asahi Glass Fluon® AD639 PTFE Aqueous Dispersion Fluon®PTFE aqueous dispersions are useful for glass cloth coating, metal coating, binder, additive in resin, feedstock of heat resistive paint ,etc.Information provided by Asahi Glass Company, Inc... |
|||
Surface Tension | 33 dynes/cm | 33 dynes/cm | Ring Method |
Asahi Glass Fluon® XAD938 PTFE Aqueous Dispersion Fluon®PTFE aqueous dispersions are useful for glass cloth coating, metal coating, binder, additive in resin, feedstock of heat resistive paint ,etc.Information provided by Asahi Glass Company, Inc... |
|||
Surface Tension | 33 dynes/cm | 33 dynes/cm | at CMC |
Solvay RHODAPEX® CO-436 Surfactant Chemical Name: AMMONIUM NONYLPHENOL ETHER SULFATECAS: 68649-55-8Available in: Asia Pacific, Europe, Latin America and North America Applications: RHODAPEX CO-436 can be used to prepare a broad range.. |