Physical Properties | Metric | English | Comments |
---|---|---|---|
Surface Tension | >= 44 dynes/cm | >= 44 dynes/cm | 1st surface; units: Dyne; Dyne Pens |
SABIC Innovative Plastics Lexan® FR83 Polycarbonate Film, Flame Retardant Lexan* FR83 flame-retardant film is a matt/polished, thin-gauge polycarbonate film with a UL94 VTM-0 listing to meet the stringent requirements in a wide range of electrical, electronic and transpor.. |
|||
Surface Tension | >= 44 dynes/cm | >= 44 dynes/cm | 1st surface; units: Dyne; Dyne Pens |
SABIC Innovative Plastics Valox® FR1 Polybutylene Terephthalate Film, Flame Retardant Valox FR-1 film is a flame retardant thermoplastic polybutylene, terephthalite film offering UL94 VTM-0 performance down to 125 microns and good temperature performance. Valox FR-1 film’s outst.. |
|||
Surface Tension | 44 dynes/cm | 44 dynes/cm | at CMC |
Solvay IGEPAL® CA 897 Surfactant Chemical Name: ETHOXYLATED OCTYLPHENOL, BRANCHED (40) CAS: 9002-93-1; 7732-18-5 Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: IGEPAL© CA-897 is an excellent pri.. |
|||
Surface Tension | 44 dynes/cm | 44 dynes/cm | at CMC |
Solvay IGEPAL® CO 880 Surfactant Identification: Nonylphenol Ethoxylate (30 EO)CAS: 68412 – 54 – 4Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: IGEPAL CO-880 is a nonionic co-emulsifier .. |
|||
Surface Tension | 44 dynes/cm | 44 dynes/cm | at CMC |
Solvay IGEPAL® CO 897 Surfactant Identification: Nonylphenol Ethoxylate (40 EO)CAS: 68412 – 54 – 4Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: IGEPAL CO-897 is a versatile emulsion poly.. |
|||
Surface Tension | 44 dynes/cm | 44 dynes/cm | at CMC |
Solvay IGEPAL® CO 897/EP Surfactant Description: Nonyl phenol based non ionic surfactant (40 EO). Emulsion polymerization grade.Chemical Name: NONYLPHENOXY POLY (ETHYLENEOXY) ETHANOL, BRANCHED, 70% ACTIVECAS: 68412-54-4, 7732-18-5 Ava.. |
|||
Surface Tension | 44 dynes/cm | 44 dynes/cm | at CMC |
Solvay IGEPAL® CO 977 Surfactant Identification: NONYLPHENOXY POLY(ETHYLENEOXY)ETHANOL, BRANCHED, 70% ACTIVECAS: 68412-54-4; 7732-18-5Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: IGEPAL© CO-97.. |
|||
Surface Tension | 44 dynes/cm | 44 dynes/cm | Harmonic Mean - Dispersive |
Eastman Embrace LV Copolyester for Shrink Film Applications:Beverage packagingDairy packagingFood packagingJuice packagingPharmaceutical packagingSoft drink packagingKey Attributes:Customizable shrink curveEye-catching 360° graphic capabilityLo.. |
|||
Surface Tension | 44 dynes/cm | 44 dynes/cm | |
BASF Pluronic® 17 R4 Block Copolymer Surfactant Description: Pluronic 17R4 is a difunctional block copolymer surfactant with terminal secondary hydroxyl groups. A nonionic surfactant that is 100% active and relatively non-toxic.Information provi.. |
|||
Surface Tension | 44 dynes/cm | 44 dynes/cm | |
Solvay Specialty Polymers Diofan® P510 Polyvinylidene Chloride (PVDC)
(discontinued **) DIOFAN® P510 is an one-component latex, water based dispersion of a polyvinylidene chloride copolymer. It is free of solvent traces, alkylphenol ethoxylates or any other toxic substances. Thanks to.. |
|||
Surface Tension | >= 44 dynes/cm | >= 44 dynes/cm | 1st surface; units: Dyne; Dyne Pens |
SABIC Innovative Plastics Lexan® FR65 Polycarbonate Film, Flame Retardant Lexan FR65 flame-retardant film is a clear, thin-gauge polycarbonate film with a velvet finish on one side and a matt finish on the other, and a UL94 V-0 listing to meet the stringent requirements i.. |
|||
Surface Tension | >= 44 dynes/cm | >= 44 dynes/cm | 2nd surface; units: Dyne; Dyne Pens |
SABIC Innovative Plastics Lexan® FR65 Polycarbonate Film, Flame Retardant Lexan FR65 flame-retardant film is a clear, thin-gauge polycarbonate film with a velvet finish on one side and a matt finish on the other, and a UL94 V-0 listing to meet the stringent requirements i.. |