Physical Properties | Metric | English | Comments |
---|---|---|---|
High Load Melt Index | 20 g/10 min @Load 21.6 kg, Temperature 200 °C |
20 g/10 min @Load 47.6 lb, Temperature 392 °F |
ISO 1133 |
Premix Thermoplastics PRE-ELEC® ESD 7100 PRE-ELEC ESD 7100 is a static dissipative thermoplastic compound based on ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7100 has been developed for inject.. |
|||
High Load Melt Index | 20 g/10 min @Load 21.6 kg |
20 g/10 min @Load 47.6 lb |
ASTM D 1238 |
Total Finathene® 3802N Natural HDPE pipe grade
(discontinued **) Applications: Natural gas distribution, extruded pipes, molded fittings, pipe coating, pipe liningInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and .. |
|||
High Load Melt Index | 20 g/10 min @Load 21.6 kg |
20 g/10 min @Load 47.6 lb |
ASTM D 1238 |
Total Finathene® CD 522 HDPE corrugated pipe resin
(discontinued **) Applications: corrugated pipe, storm and sanitary sewers, drainage systemsInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics produc.. |
|||
High Load Melt Index | 20 g/10 min @Load 21.6 kg |
20 g/10 min @Load 47.6 lb |
ASTM D 1238 |
Total Finathene® DF 210 HDPE resin
(discontinued **) Applications: Irrigation tape and tubingInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines. |
|||
High Load Melt Index | 20 g/10 min @Load 21.6 kg, Temperature 190 °C |
20 g/10 min @Load 47.6 lb, Temperature 374 °F |
High Load; ASTM D1238 |
Chevron Phillips Marlex® HHM TR-418N/M358Y Natural medium density ethylene hexene copolymer/yellow concrete
( Benefits: environmentally-friendly pigment system, yellow color for easy identification, outstanding pipe rind ESCR, UV stabilizer in natural resin, concentrate base resinCharacteristics: Pipe Ring .. |
|||
High Load Melt Index | 20 g/10 min @Load 21.6 kg, Temperature 190 °C |
20 g/10 min @Load 47.6 lb, Temperature 374 °F |
|
Meilian Chemical PE305A RED MASTERBATCH RED PE 305A is a red LDPE-based masterbatch containing 32% pigment, designed for use in polyolefin resins (PE and PP, etc..). Color Index No.: Red 53:1Method of Usage: RED PE 305A is designed for ea.. |
|||
High Load Melt Index | 20 g/10 min @Load 21.6 kg |
20 g/10 min @Load 47.6 lb |
ASTM D 1238 |
Total CD 4300 HDPE extrusion Applications: General profile extrusion, irradiation-crosslinked productsInformation provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product.. |
|||
High Load Melt Index | 20 g/10 min @Load 21.6 kg |
20 g/10 min @Load 47.6 lb |
ASTM D 1238 |
Total HL 428 HDPE film resin Applications: multi-wall liner, poultry multi-layer gas flush bags, mailing envelopes, heavy-duty shipping sacks, fresh cut produce packaging, coextrusionInformation provided provided by Total Petro.. |
|||
High Load Melt Index | 20 g/10 min @Load 21.6 kg, Temperature 190 °C |
20 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Formosa Plastics Formolene® HF3728 Film (Hexene) HDPE High Density Polyethylene Medium Molecular weight Film Resin Formolene® HF3728 is a medium density resin that provides an excellent overall balance of tensile, impact, and tear properties in thin f.. |
|||
High Load Melt Index | 20 g/10 min @Load 21.6 kg, Temperature 190 °C |
20 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |
Borealis Borstar® FB2310 LLDPE for Film Borstar BF2310 is a high molecular weight low density polyethylene film grade combining good and flexible extrusion behavior, excellent draw down and superior mechanical properties. Film made from .. |
|||
High Load Melt Index | 20 g/10 min @Load 21.6 kg, Temperature 190 °C |
20 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Total HL 428 HDPE Film Grade Medium molecular weight grade. Excellent processability, excellent compatibility with LDPE and LLDPE, good tear and impact strength, good stiffness, excellent drawdown, and good moisture barrier pro.. |
|||
High Load Melt Index | 20 g/10 min @Load 21.6 kg, Temperature 190 °C |
20 g/10 min @Load 47.6 lb, Temperature 374 °F |
HLMI; ASTM D1238 |
Chevron Phillips MarFlex® HHM TR-130 MDPE Film Resin Medium density resin provides overall balance of tensile, impact, and tear properties in film. It is suited for merchandise, produce, and trash bags. Processing performance is excellent on high st.. |
|||
High Load Melt Index | 20 g/10 min @Load 21.6 kg, Temperature 190 °C |
20 g/10 min @Load 47.6 lb, Temperature 374 °F |
High Load; ASTM D1238 |
Chevron Phillips Marlex® HHM TR-418Q MDPE Hexene Copolymer High performance MDPE resin has been formulated for the demanding requirements of pressure pipe applications. Meets ASTM D4976 PE 225. Meets FDA Regulation 177.1520, suitable for food packaging ap.. |
|||
High Load Melt Index | 20 g/10 min @Load 21.6 kg, Temperature 190 °C |
20 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Dow DFDC-7525 NT High Density Polyethylene Resin DOW DFDC-7525 NT is produced using UNIPOL™ process technology. It is intended for use in thin wall drip tape and micro-irrigation tube, hose and tube, and profile extrusion applications. Informati.. |
|||
High Load Melt Index | 20 g/10 min @Load 21.6 kg, Temperature 190 °C |
20 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Dow FLEXOMER™ DFDA-1010 NT 7 Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ DFDA-1010 NT 7 is an ethylene-butene copolymer produced via gas phase polymerization from Dow. It can be utilized in monolayer and co-extruded films and in blends with other polyolefins .. |
|||
High Load Melt Index | 20 g/10 min @Load 21.6 kg, Temperature 190 °C |
20 g/10 min @Load 47.6 lb, Temperature 374 °F |
HLMI; ASTM D1238 |
Bapolene® 345F Medium Density Polyethylene Film Resin Description: Bapolene 345F is a medium molecular weight film resin with excellent tensile, impact, and tear properties. Applications: Merchandise bags, produce and trash bags.Bapolene® and Bapolan®.. |
|||
High Load Melt Index | 20 g/10 min @Load 21.6 kg |
20 g/10 min @Load 47.6 lb |
ASTM D 1238 |
Total Finathene® HL 328 HDPE resin
(discontinued **) Applications: Specialty merchandise bags, millinery/notion bags, mailing envelopes, heavy-duty shipping sacks, shrink films, fresh cut produce packaging, coextrusionInformation provided provided by .. |
|||
High Load Melt Index | 20 g/10 min @Load 21.6 kg |
20 g/10 min @Load 47.6 lb |
ASTM D 1238 |
Total CD 471 HDPE conduit Applications: Wire and cable conduit, fiber optic innerductInformation provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines. |
|||
High Load Melt Index | 20 g/10 min @Load 21.6 kg, Temperature 190 °C |
20 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Formosa Plastics Formolene® HP3902 Pipe HDPE Natural Medium Density Hexene CopolymerApplications: Pipe for gas distribution, oilfield and other industrial pipe, telecommunications conduit.Formolene HP3902 is a high performance copolymer that i.. |