Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Test | 150 - 250 cm³/g | 150 - 250 cm³/g | Average value: 203 cm³/g Grade Count:9 |
Overview of materials for Nylon 66/6 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb .. |
|||
Viscosity Test | 150 - 205 cm³/g | 150 - 205 cm³/g | Average value: 178 cm³/g Grade Count:4 |
Overview of materials for Nylon 66, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum .. |
|||
Viscosity Test | 150 - 170 cm³/g | 150 - 170 cm³/g | Average value: 157 cm³/g Grade Count:3 |
Overview of materials for Nylon 610 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | H<sub>2</sub>SO<sub>4</sub>; ISO 307 |
Sax Polymers SAXAMID 126F4RZ21 Nylon 6, 20% Glass Fiber SAXAMID 126F4RZ21 is a polyamide 6 injection-molding-grade reinforced with 20% glass fibers. It is equipped with a halogen-free and phosphorus-free flame retardant.Information provided by SAX Polyme.. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | H<sub>2</sub>SO<sub>4</sub>; ISO 307 |
Sax Polymers SAXAMID 126F6RY01 Nylon 6, 30% Glass Fiber SAXAMID 126F6RY01 is a polyamide 6 injection-molding-grade reinforced with 30% glass fibers. It has a halogen-free flame retardant.Information provided by SAX Polymers |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | H<sub>2</sub>SO<sub>4</sub>; ISO 307 |
Sax Polymers SAXAMID 126F4 Nylon 6, 20% Glass Fiber SAXAMID 126F4 is a polyamide 6 injection-molding-grade reinforced with 20% glass fibers.Information provided by SAX Polymers |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | H<sub>2</sub>SO<sub>4</sub>; ISO 307 |
Sax Polymers SAXAMID 126H Nylon 6, Injection Molding Grade SAXAMID 126H is a general purpose polyamide 6 injection-molding-grade. Benefits are short cycle times and good release properties. Additionally it has a higher content of heat stabilizer which is p.. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | H<sub>2</sub>SO<sub>4</sub>; ISO 307 |
Sax Polymers SAXAMID 126K6 Nylon 6, 30% Glass Filled SAXAMID 126K6 is a 30% glass beads filled polyamide 6 injection-molding-grade. It is characterized by dimensional stability, low warpage and good surface quality.Information provided by SAX Polymers.. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | H<sub>2</sub>SO<sub>4</sub>; ISO 307 |
Sax Polymers SAXAMID 136F6Q32 Nylon 6, 30% Glass Fiber SAXAMID 136F6Q32 is a high-impact-modified polyamide 6 injection-molding-grade reinforced with 30% glass fibers . Beside the high impact strength at low temperatures this grade shows very good proce.. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | H<sub>2</sub>SO<sub>4</sub>; ISO 307 |
Sax Polymers SAXAMID 226F10 Nylon 6.6, 50% Glass Fiber SAXAMID 226F10 is a polyamide 6.6 injection-molding-grade reinforced with 50% glass fibers. It has high mechanical strength.Information provided by SAX Polymers |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | H<sub>2</sub>SO<sub>4</sub>; ISO 307 |
Sax Polymers SAXAMID 226F3 Nylon 6.6, 15% Glass Fiber SAXAMID 226F3 is a polyamide 6.6 injection-molding-grade reinforced with 15% glass fibers. This grade is suitable for applications requiring high strength and very good flow properties during proces.. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | H<sub>2</sub>SO<sub>4</sub>; ISO 307 |
Sax Polymers SAXAMID 226F6RY01 Nylon 6.6, 30% Glass Fiber SAXAMID 226F6RY01 is a polyamide 6.6 injection-molding-grade reinforced with 30% glass fibers. It has a halogen-free flame retardant.Information provided by SAX Polymers |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | H<sub>2</sub>SO<sub>4</sub>; ISO 307 |
Sax Polymers SAXAMID 226F7 Nylon 6.6, 35% Glass Fiber SAXAMID 226F7 is a general purpose polyamide 6.6 injection-molding-grade reinforced with 35% glass fibers. It has very high mechanical strength in combination with good impact resistance. It is char.. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | H<sub>2</sub>SO<sub>4</sub>; ISO 307 |
Sax Polymers SAXAMID 126 Nylon 6, Injection Molding Grade SAXAMID 126 is a general purpose polyamide 6 injection-molding-grade. Benefits are short cycle times and good release properties.Information provided by SAX Polymers |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | H<sub>2</sub>SO<sub>4</sub>; ISO 307 |
Sax Polymers SAXAMID 126F5 Nylon 6, 25% Glass Fiber SAXAMID 126F5 is a polyamide 6 injection-molding-grade reinforced with 25% glass fibers.Information provided by SAX Polymers |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | Viscosity Number |
DSM Stanyl® TE250F8 Nylon 46-40% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | DAM; ISO 307 1157 1628 |
DuPont Performance Polymers Zytel® 70G35HSRX BK099 Nylon 66
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G35HSRX BK099 a 35% glass reinforced heat stabilized hydrolysis resistant PA66 for injection molding. Developed for applications designed fo.. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | DAM; ISO 307 1157 1628 |
DuPont Performance Polymers Zytel® 7335F NC010 Nylon 6
(Unverified Data**) Unreinforced Polyamide 6 Zytel 7335F NC010 is a nucleated lubricated polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | DAM; ISO 307 1157 1628 |
DuPont Performance Polymers Zytel® 73G30HSL BK416 Nylon 6
(Unverified Data**) 30% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G30HSL BK416 is a 30% glass fiber reinforced heat stabilized lubricated black polyamide 6 resin for injection molding.Information provided by.. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | DAM; ISO 307 1157 1628 |
DuPont Performance Polymers Zytel® RS LC3060 NC010 Nylon 610
(Unverified Data**) Unreinforced Renewably Sourced Medium Viscosity Polyamide 610 Developed for Extrusion Zytel RS LC3060 NC010 is a renewable sourced polyamide 610 containing a minimum of 60% renewable sourced ingredi.. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | Viscosity Number; ISO 307, 1157, 1628 |
DSM EcoPaXX® Q150-D PA410 Low/Medium Viscosity |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | DAM; ISO 307 1157 1628 |
DuPont Performance Polymers Minlon® 73GM40 NC010 Nylon 6
(Unverified Data**) 40% Mineral/Glass Reinforced Polyamide 6 Minlon 73GM40 NC010 is a 40% mineral/glass reinforced heat stabilized polyamide 6 resin for injection molding.Information provided by DuPont Performance Poly.. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | DAM; ISO 307 1157 1628 |
DuPont Performance Polymers Zytel® 135F NC010 Nylon 66
(Unverified Data**) Unreinforced Nucleated Polyamide 66 Zytel 135F NC010 is a nucleated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Pe.. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | DAM; ISO 307 1157 1628 |
DuPont Performance Polymers Zytel® 70G13L NC010 Nylon 66
(Unverified Data**) 13% Glass Reinforced Polyamide 66Zytel 70G13L NC010 is a 13% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | 0.5% in 96% H2SO4; ISO 307 |
Azoty Tarnow™ Alphalon™ 27D Nylon 6 A bright polyamide 6 grade of low viscosity suited for the production of compounds.Information provided by ATT Polymers™ |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | Viscosity number |
BASF Ultramid® B3S Q661 PA6 (Dry) Ultramid B3S Q661 is a general purpose, PA6 resin for injection molding. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | Viscosity number |
BASF Ultramid® B3M6 30% Mineral Filled PA6 (Dry) Ultramid B3M6 is a 30% mineral reinforced injection molding PA6 grade for industrial items requiring high impact strength and very high dimensional stability, excellent laser markability. |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | DAM; ISO 307 1157 1628 |
DuPont Performance Polymers Zytel® 70G30HSL BK039B Nylon 66
(Unverified Data**) 30% Glass Reinforced Heat Stabilized Polyamide 66 Information provided by DuPont Performance Polymers |
|||
Viscosity Test | 150 cm³/g | 150 cm³/g | H<sub>2</sub>SO<sub>4</sub>; ISO 307 |
Sax Polymers SAXAMID 236Q33 Nylon 6.6, Impact Modified SAXAMID 236Q33 is a impact-modified polyamide 6.6 injection-molding-grade with very good flow properties and outstanding toughness. Even at low temperatures this grade offers super-tough properties... |