Physical Properties Metric English Comments
Viscosity Test 2600 cm³/g
2600 cm³/g
Intrinsic; ASTM D4020
LyondellBasell Montell 1900 UHMW Polyethylene
Key Features: ultrahigh molecular weight polyethylene resin, excellent abrasion resistance, high impact strength, low coefficient of friction, good chemical resistance, low odor and taste transferAp..
Viscosity Test 2600 cm³/g
2600 cm³/g
Intrinsic; ASTM D4020
LyondellBasell Montell 1900CM UHMW Polyethylene
Key Features: ultrahigh molecular weight polyethylene resin, excellent abrasion resistance, high impact strength, low coefficient of fraction, good chemical resistance, low odor and taste transfer, ..