Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Test | 2800 cm³/g | 2800 cm³/g | Intrinsic; ASTM D4020 |
LyondellBasell Montell HB320CM UHMW Polyethylene Key Features: ultrahigh molecular weight polyethylene resin, excellent abrasion resistance, high impact strength, low coefficient of friction, good chemical resistance, low odor and taste transfer, .. |