Physical Properties Metric English Comments
Viscosity Test 63 - 65 cm³/g
63 - 65 cm³/g
Ubbelhode
Iran Petrochemical (PCC) TG 641 Polyethylene Terephthalate
Polyethylene Terephthalate fiber grade chips, semi dullApplications: staple fiber, textile filament, spunbond, meltblown nonwovensInformation provided by Iran Petrochemical Commercial Co.
Viscosity Test 63 - 65 cm³/g
63 - 65 cm³/g
Ubbelhode
Iran Petrochemical (PCC) TG 641 Super Bright Polyethylene Terephthalate
Polyethylene Terephthalate fiber grade chips, super brightApplications: staple fiber, textile filament, spunbond, meltblown nonwovensInformation provided by Iran Petrochemical Commercial Co.
Viscosity Test 63 - 65 cm³/g
63 - 65 cm³/g
Ubbelhode
Iran Petrochemical (PCC) TG 645 Super Bright Polyethylene Terephthalate
Polyethylene Terephthalate fiber grade chips, super brightInformation provided by Iran Petrochemical Commercial Co.
Viscosity Test 63 cm³/g
63 cm³/g
Viscosity Number
Mitsubishi Xantar® 25 R Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Viscosity Test 63 cm³/g
63 cm³/g
Viscosity Number
Mitsubishi Xantar® 25 SR FD Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Viscosity Test 63 cm³/g
63 cm³/g
Viscosity Number
Mitsubishi Xantar® 25 UR Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Viscosity Test 63 cm³/g
63 cm³/g
Viscosity Number
Mitsubishi Xantar® F 25 R Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Viscosity Test 63 cm³/g
63 cm³/g
Viscosity Number
Mitsubishi Xantar® FC 25 R Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Viscosity Test 63 cm³/g
63 cm³/g
Viscosity Number
Mitsubishi Xantar® FC 25 UR Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Viscosity Test 63 cm³/g
63 cm³/g
Viscosity Number
Mitsubishi Xantar® F 25 UR Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Viscosity Test 63 cm³/g
63 cm³/g
Viscosity number
BASF Ultrason S 2010 G4 20% Glass Filled PSU
Ultrason S 2010 G4 is a 20% glass reinforced, medium viscosity injection molding PSU grade with high rigidity and strength.
Viscosity Test 63 cm³/g
63 cm³/g
Viscosity number
BASF Ultrason S 2010 G6 30% Glass Filled PSU
Ultrason S 2010 G6 is a 30% glass reinforced, medium viscosity injection molding PSU grade with high rigidity and strength.
Viscosity Test 63 cm³/g
63 cm³/g
Viscosity number
BASF Ultrason S 2010 PSU
Ultrason S 2010 is an unreinforced, medium viscosity standard injection molding PSU grade. It flows readily and offers outstanding heat resistance and dimensional stability. It conforms to FDA req..
Viscosity Test 63 - 65 cm³/g
63 - 65 cm³/g
Ubbelhode
Iran Petrochemical (PCC) TG 645 Polyethylene Terephthalate
Polyethylene Terephthalate fiber grade chipsInformation provided by Iran Petrochemical Commercial Co.
Copyright © lookpolymers.com All Rights Reserved