Polymer Property : ESCR 100% Igepal® = 1.0 hour Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
ESCR 100% Igepal® <= 1.0 hour
<= 1.0 hour
F50; ASTM D1693B
SABIC M300054 High Density Polyethylene for Injection Molding
Product Description: M300054 is a high density polyethylene grade with a narrow molecular weight distribution suitable for injection molding applications. It has been designed to provide good flow..
ESCR 100% Igepal® 1.0 hour

@Thickness 3.00 mm,
Temperature 23.0 °C
1.0 hour

@Thickness 0.118 in,
Temperature 73.4 °F
compression molded plaques; ASTM D1693
Braskem BI 818 LDPE Injection Molding Polyethylene  (discontinued **)
Applications: Injection molding; masterbatches. Information provided by Braskem
ESCR 100% Igepal® 1.0 hour
1.0 hour
Condition B; ASTM D1693
A. Schulman LP481 Molding Grade High-Density Polyethylene
DescriptionLP 481 is a molding grade high-density polyethylene. Information provided by A. Schulman.
ESCR 100% Igepal® 1.0 hour
1.0 hour
Condition B; ASTM D1693
A. Schulman LP552-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene
DescriptionLP 552-01 is a U.L. approved narrow molecular weight copolymer high-density polyethylene combining good flow with excellent stiffness and cold temperature impact strength. It has good tou..
ESCR 100% Igepal® 1.0 hour
1.0 hour
Condition B; ASTM D1693
A. Schulman LP554-01 Narrow Molecular Weight Homopolymer, High-Density Polyethylene
DescriptionLP 554-01 is a narrow molecular weight homopolymer high-density polyethylene exhibiting toughness, rigidity and warpage resistance. ApplicationApplications of LP 554-01 include crates, t..
ESCR 100% Igepal® 1.0 hour
1.0 hour
Condition B; ASTM D1693
A. Schulman LP481 Molding Grade High-Density Polyethylene
DescriptionLP 481 is a molding grade high-density polyethylene. Information provided by A. Schulman.
ESCR 100% Igepal® 1.0 hour
1.0 hour
Condition B; ASTM D1693
A. Schulman LP552-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene
DescriptionLP 552-01 is a U.L. approved narrow molecular weight copolymer high-density polyethylene combining good flow with excellent stiffness and cold temperature impact strength. It has good tou..
ESCR 100% Igepal® 1.0 hour
1.0 hour
Condition B; ASTM D1693
A. Schulman LP554-01 Narrow Molecular Weight Homopolymer, High-Density Polyethylene
DescriptionLP 554-01 is a narrow molecular weight homopolymer high-density polyethylene exhibiting toughness, rigidity and warpage resistance. ApplicationApplications of LP 554-01 include crates, t..
ESCR 100% Igepal® 1.0 hour
1.0 hour
Condition B; ASTM D1693
A. Schulman LP481 Molding Grade High-Density Polyethylene
DescriptionLP 481 is a molding grade high-density polyethylene. Information provided by A. Schulman.
ESCR 100% Igepal® 1.0 hour
1.0 hour
Condition B; ASTM D1693
A. Schulman LP552-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene
DescriptionLP 552-01 is a U.L. approved narrow molecular weight copolymer high-density polyethylene combining good flow with excellent stiffness and cold temperature impact strength. It has good tou..
ESCR 100% Igepal® 1.0 hour
1.0 hour
Condition B; ASTM D1693
A. Schulman LP554-01 Narrow Molecular Weight Homopolymer, High-Density Polyethylene
DescriptionLP 554-01 is a narrow molecular weight homopolymer high-density polyethylene exhibiting toughness, rigidity and warpage resistance. ApplicationApplications of LP 554-01 include crates, t..
ESCR 100% Igepal® 1.0 hour
1.0 hour
Condition B; ASTM D1693
A. Schulman LP481 Molding Grade High-Density Polyethylene
DescriptionLP 481 is a molding grade high-density polyethylene. Information provided by A. Schulman.
ESCR 100% Igepal® 1.0 hour
1.0 hour
Condition B; ASTM D1693
A. Schulman LP552-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene
DescriptionLP 552-01 is a U.L. approved narrow molecular weight copolymer high-density polyethylene combining good flow with excellent stiffness and cold temperature impact strength. It has good tou..
ESCR 100% Igepal® 1.0 hour
1.0 hour
Condition B; ASTM D1693
A. Schulman LP554-01 Narrow Molecular Weight Homopolymer, High-Density Polyethylene
DescriptionLP 554-01 is a narrow molecular weight homopolymer high-density polyethylene exhibiting toughness, rigidity and warpage resistance. ApplicationApplications of LP 554-01 include crates, t..
ESCR 100% Igepal® 1.0 hour
1.0 hour
Condition B; ASTM D1693
A. Schulman LP552-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene
DescriptionLP 552-01 is a U.L. approved narrow molecular weight copolymer high-density polyethylene combining good flow with excellent stiffness and cold temperature impact strength. It has good tou..
ESCR 100% Igepal® 1.0 hour
1.0 hour
Condition B; ASTM D1693
A. Schulman LP554-01 Narrow Molecular Weight Homopolymer, High-Density Polyethylene
DescriptionLP 554-01 is a narrow molecular weight homopolymer high-density polyethylene exhibiting toughness, rigidity and warpage resistance. ApplicationApplications of LP 554-01 include crates, t..
ESCR 100% Igepal® 1.0 hour
1.0 hour
Condition B; ASTM D1693
A. Schulman LP552-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene
DescriptionLP 552-01 is a U.L. approved narrow molecular weight copolymer high-density polyethylene combining good flow with excellent stiffness and cold temperature impact strength. It has good tou..
ESCR 100% Igepal® 1.0 hour
1.0 hour
Condition B; ASTM D1693
A. Schulman LP554-01 Narrow Molecular Weight Homopolymer, High-Density Polyethylene
DescriptionLP 554-01 is a narrow molecular weight homopolymer high-density polyethylene exhibiting toughness, rigidity and warpage resistance. ApplicationApplications of LP 554-01 include crates, t..
ESCR 100% Igepal® 1.0 hour
1.0 hour
Condition B; ASTM D1693
A. Schulman LP481 Molding Grade High-Density Polyethylene
DescriptionLP 481 is a molding grade high-density polyethylene. Information provided by A. Schulman.
ESCR 100% Igepal® <= 1.0 hour

@Temperature 50.0 °C
<= 1.0 hour

@Temperature 122 °F
F<sub>50</sub>; Compression molded; ASTM D1693
Dow 620I Linear Low Density Polyethylene (LDPE)
For extruded foam applications Complies with U.S. FDA 21 CFR 177.1520 (c) 2.1 Information provided by Dow
ESCR 100% Igepal® <= 1.0 hour

@Temperature 50.0 °C
<= 1.0 hour

@Temperature 122 °F
F<sub>50</sub>; Molded and tested in accordance with ASTM D4976; ASTM D1693
Dow 722 Linear Low Density Polyethylene (LDPE)
DOW Polyethylene 722 is a broad molecular weight distribution homopolymer designed to offer good impact strength and rack resistance, with excellent flexibility. Typical applications include caps/c..
ESCR 100% Igepal® <= 1.0 hour

@Temperature 50.0 °C
<= 1.0 hour

@Temperature 122 °F
F<sub>50</sub>; Molded and tested in accordance with ASTM D4976; ASTM D1693
Dow DNDA-9810 NT 7 Linear Low Density Polyethylene Resin
DOW DNDA-9810 NT 7 is produced using UNIPOL™ PE process technology and is supplied in pellet form. This resin is specifically designed as a carrier resin for color concentrates and other masterbat..
ESCR 100% Igepal® <= 1.0 hour

@Temperature 50.0 °C
<= 1.0 hour

@Temperature 122 °F
F<sub>50</sub>; Molded and tested in accordance with ASTM D4976; ASTM D1693
Dow 959S Linear Low Density Polyethylene (LDPE)
DOW Polyethylene 959S is a medium molecular weight distribution homopolymer. This resin has good process-ability over a wide range of molding conditions. Typical applications include lids. It com..
ESCR 100% Igepal® <= 1.0 hour

@Temperature 50.0 °C
<= 1.0 hour

@Temperature 122 °F
F<sub>50</sub>; Molded and tested in accordance with ASTM D4976; ASTM D1693
Dow DNDB-1077 NT 7 Linear Low Density Polyethylene Resin
DOW DNDB-1077 NT 7 is produced using UNIPOL™ PE process technology. It is intended for high-speed injection molding of thin walled parts such as downguaged lids. Information provided by Dow
ESCR 100% Igepal® 1.0 hour
1.0 hour
Condition B; ASTM D1693
A. Schulman LP481 Molding Grade High-Density Polyethylene
DescriptionLP 481 is a molding grade high-density polyethylene. Information provided by A. Schulman.