Physical Properties | Metric | English | Comments |
---|---|---|---|
ESCR 100% Igepal® | 300 hour | 300 hour | ASTM D1693 |
ExxonMobil LL 8555.24 Rotational Molding Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |
|||
ESCR 100% Igepal® | 300 hour | 300 hour | ASTM D1693 |
ExxonMobil LL 8555.25 Rotational Molding Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |
|||
ESCR 100% Igepal® | 300 hour | 300 hour | ASTM D1693 |
ExxonMobil LLP8555.24 Rotational Molding Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |
|||
ESCR 100% Igepal® | 300 hour | 300 hour | ASTM D1693 |
ExxonMobil LLP8555.25 Rotational Molding Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |
|||
ESCR 100% Igepal® | >= 300 hour @Thickness 2.00 mm, Temperature 50.0 °C |
>= 300 hour @Thickness 0.0787 in, Temperature 122 °F |
0.3 mm notched-plaques; ASTM-D1693 |
Braskem Evateno® 3019 PE EVA Foam Copolymer Evateno® 3019 PE is a copolymer of Ethylene-Vinyl Acetate (EVA) with medium vinyl-acetate content. Evateno® 3019 PE is an easy processing and crosslinkable product with high compatibility with oth.. |
|||
ESCR 100% Igepal® | >= 300 hour @Thickness 2.00 mm, Temperature 50.0 °C |
>= 300 hour @Thickness 0.0787 in, Temperature 122 °F |
0.3 mm notched-plaques; ASTM-D1693 |
Braskem Evateno® 8019 PE EVA Foam Copolymer The Evateno® 8019 PE is a copolymer of Ethylene-Vinyl Acetate (EVA) with medium Vinyl-Acetate content. Evateno® 8019 PE is an easy processing and crosslinkable product with high compatibility with.. |
|||
ESCR 100% Igepal® | >= 300 hour @Thickness 2.00 mm, Temperature 50.0 °C |
>= 300 hour @Thickness 0.0787 in, Temperature 122 °F |
0.3 mm notched-plaques; ASTM-D1693 |
Braskem Evateno® HM 150 EVA Hot Melt Copolymer Evateno® HM 150 is a copolymer of Ethylene-Vinyl Acetate (EVA) with medium vinyl-acetate content, very low molecular weight, and easy crosslinkability. Evateno® HM-150 offers good compatibility wi.. |
|||
ESCR 100% Igepal® | >= 300 hour @Thickness 2.00 mm, Temperature 50.0 °C |
>= 300 hour @Thickness 0.0787 in, Temperature 122 °F |
0.3 mm notched-plaques; ASTM-D1693 |
Braskem Evateno® HM 2528 EVA Hot Melt Copolymer Evateno® HM 2528 is a copolymer of Ethylene-Vinyl Acetate (EVA) with high vinyl-acetate content, low molecular weight, and good compatibility with other thermoplastic and elastomeric resins, and it.. |
|||
ESCR 100% Igepal® | >= 300 hour @Thickness 2.00 mm, Temperature 50.0 °C |
>= 300 hour @Thickness 0.0787 in, Temperature 122 °F |
0.3 mm notched-plaques; ASTM-D1693 |
Braskem Evateno® HM 728 EVA Hot Melt Copolymer Evateno® HM 728 is a copolymer of Ethylene-Vinyl Acetate (EVA) with high vinyl-acetate content, medium molecular weight, and good compatibility with other thermoplastic and elastomeric resins. Evat.. |
|||
ESCR 100% Igepal® | 300 hour @Thickness 2.00 mm, Temperature 50.0 °C |
300 hour @Thickness 0.0787 in, Temperature 122 °F |
0.3 mm notched-plaques; ASTM-D1693 |
Braskem ML4400N LLDPE Rotomolding Polyethylene The resin ML4400N is a linear low-density polyethylene, 1-butene based, with high stiffness and an adequate balance of processability and environmental stress cracking resistance. It contains long t.. |
|||
ESCR 100% Igepal® | 300 hour @Thickness 2.00 mm, Temperature 50.0 °C |
300 hour @Thickness 0.0787 in, Temperature 122 °F |
0.3 mm notched-plaques; ASTM-D1693 |
Braskem RC35U4 LLDPE Rotomolding Polyethylene The resin RC35U4 is a linear low-density polyethylene, 1-butene based, with high stiffness and an adequate balance of processability and environmental stress cracking resistance. It contains long te.. |
|||
ESCR 100% Igepal® | >= 300 hour @Thickness 2.00 mm, Temperature 50.0 °C |
>= 300 hour @Thickness 0.0787 in, Temperature 122 °F |
0.3 mm notched-plaques; ASTM-D1693 |
Braskem VA2019A EVA Foam Copolymer The VA2019A is a copolymer of Ethylene-Vinyl Acetate (EVA) with medium vinyl-acetate content. VA2019A is an easy processing product with high compatibility with other thermoplastic and elastomeric r.. |