Physical Properties | Metric | English | Comments |
---|---|---|---|
ESCR 100% Igepal® | 5.0 hour | 5.0 hour | Condition B; ASTM D1693 |
A. Schulman LP551-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP551-01 is a narrow molecular weight copolymer, high-density polyethylene combining excellent impact strength with good environmental stress crack resistance. ApplicationApplications of.. |
|||
ESCR 100% Igepal® | 5.0 hour | 5.0 hour | Condition B; ASTM D1693 |
A. Schulman LP390-01 Narrow Molecular Weight Copolymer DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-0.. |
|||
ESCR 100% Igepal® | 5.0 hour | 5.0 hour | Condition B; ASTM D1693 |
A. Schulman LP551-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP551-01 is a narrow molecular weight copolymer, high-density polyethylene combining excellent impact strength with good environmental stress crack resistance. ApplicationApplications of.. |
|||
ESCR 100% Igepal® | 5.0 hour | 5.0 hour | Condition B; ASTM D1693 |
A. Schulman LP390-01 Narrow Molecular Weight Copolymer DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-0.. |
|||
ESCR 100% Igepal® | 5.0 hour | 5.0 hour | Condition B; ASTM D1693 |
A. Schulman LP551-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP551-01 is a narrow molecular weight copolymer, high-density polyethylene combining excellent impact strength with good environmental stress crack resistance. ApplicationApplications of.. |
|||
ESCR 100% Igepal® | 5.0 hour | 5.0 hour | Condition B; ASTM D1693 |
A. Schulman LP390-01 Narrow Molecular Weight Copolymer DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-0.. |
|||
ESCR 100% Igepal® | 5.0 hour | 5.0 hour | Condition B; ASTM D1693 |
A. Schulman LP551-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP551-01 is a narrow molecular weight copolymer, high-density polyethylene combining excellent impact strength with good environmental stress crack resistance. ApplicationApplications of.. |
|||
ESCR 100% Igepal® | 5.0 hour | 5.0 hour | Condition B; ASTM D1693 |
A. Schulman LP390-01 Narrow Molecular Weight Copolymer DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-0.. |
|||
ESCR 100% Igepal® | 5.0 hour | 5.0 hour | Condition B; ASTM D1693 |
A. Schulman LP551-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP551-01 is a narrow molecular weight copolymer, high-density polyethylene combining excellent impact strength with good environmental stress crack resistance. ApplicationApplications of.. |
|||
ESCR 100% Igepal® | 5.0 hour | 5.0 hour | Condition B; ASTM D1693 |
A. Schulman LP390-01 Narrow Molecular Weight Copolymer DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-0.. |
|||
ESCR 100% Igepal® | 5.0 hour | 5.0 hour | Condition B; ASTM D1693 |
A. Schulman LP390-01 Narrow Molecular Weight Copolymer DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-0.. |
|||
ESCR 100% Igepal® | 5.0 hour @Temperature 50.0 °C |
5.0 hour @Temperature 122 °F |
F<sub>50</sub>; Molded and tested in accordance with ASTM D4976; ASTM D1693 |
Dow DNDA-7147 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-7147 NT 7 is produced using UNIPOL™ PE process technology. It is intended for use in injection molding applications such as food containers, housewares and lids. Information provided by D.. |
|||
ESCR 100% Igepal® | 5.0 hour @Temperature 50.0 °C |
5.0 hour @Temperature 122 °F |
F<sub>50</sub>; Molded and tested in accordance with ASTM D4976; ASTM D1693 |
Dow DNDA-8350 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-8350 NT 7 is produced using UNIPOL™ PE process technology. It is intended for use in general purpose injection molding applications. Information provided by Dow |
|||
ESCR 100% Igepal® | <= 5.0 hour @Temperature 50.0 °C |
<= 5.0 hour @Temperature 122 °F |
h/F50; Compression molded 2mm notched-plaques; ASTM D1693 |
Braskem Green PE SHD7255LSL Injection Molding High Density Polyethylene Description: SHC7260LS-L is a high-density polyethylene, developed for the injection molding which presents high hardness and stiffness, besides low tendency to warpage. This resin has additives aga.. |
|||
ESCR 100% Igepal® | 5.0 hour | 5.0 hour | Condition B; ASTM D1693 |
A. Schulman LP551-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP551-01 is a narrow molecular weight copolymer, high-density polyethylene combining excellent impact strength with good environmental stress crack resistance. ApplicationApplications of.. |
|||
ESCR 100% Igepal® | <= 5.0 hour @Thickness 2.00 mm, Temperature 50.0 °C |
<= 5.0 hour @Thickness 0.0787 in, Temperature 122 °F |
0.3 mm notched-plaques; ASTM-D1693 |
Braskem HD7255LS-L HDPE Injection Molding Polyethylene HD7255LS-L is a high-density polyethylene developed for injection molding. It has good tenacity and impact properties combined with good stiffness. It presents a ratio between melt flow and density .. |