Physical Properties Metric English Comments
ESCR 10% Igepal® >= 1500 hour
>= 1500 hour
F50 Conditions C & B; ASTM D1693
Polymer Industries Densetec LDPE Sheet
Polymer Industries Densetec LDPE is a material that`s soft, flexible, and tough, even at low temperatures. Because of the fact that Densetec LDPE has very good formability traits and is very pliable..
ESCR 10% Igepal® >= 1500 hour
>= 1500 hour
Condition B, F<sub>50</sub>; ASTM D1693
Formosa Plastics Formolene® HL3812 Film (Hexene) HDPE
Medium Density Polyethylene Formolene® HL3812 is a high molecular weight hexene copolymer resin that is tailored specifically for geomembrane applications. The resin provides an excellent balance o..
ESCR 10% Igepal® >= 1500 hour
>= 1500 hour
Condition B; ASTM D1693
Chevron Phillips Marlex® K203 LLDPE Sheet Extrusion
Resin Type: Hexene CopolymerCharacteristics: Outstanding ESCRBroad fusion rangeExcellent melt strengthGood processabilityExcellent flexibilityImproved output and texturingApplications: Coextruded ca..