Polymer Property : ESCR 10% Igepal® = 60 hour Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
ESCR 10% Igepal® 60 hour
60 hour
F50; ASTM D1693B
SABIC B5429/B5429A High Density Polyethylene for Blow Molding
Product Description: B5429 Series grades are medium molecular weight High Density Polyethylene copolymer. They are primarily intended for blow molding articles of small sizes. B5429 series grades..
ESCR 10% Igepal® 60 hour
60 hour
ASTM D1693
ExxonMobil LL 8555.24 Rotational Molding Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
ESCR 10% Igepal® 60 hour
60 hour
ASTM D1693
ExxonMobil LL 8555.25 Rotational Molding Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
ESCR 10% Igepal® 60 hour
60 hour
F50; ASTM D1693B
ExxonMobil LLDPE LL 8555.24 Linear Low Density Polyethylene Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
ESCR 10% Igepal® 60 hour
60 hour
F50; ASTM D1693B
ExxonMobil LLDPE LL 8555.25 Linear Low Density Polyethylene Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
ESCR 10% Igepal® 60 hour
60 hour
F50; ASTM D1693B
ExxonMobil LLDPE LLP 8555.24 Linear Low Density Polyethylene Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
ESCR 10% Igepal® 60 hour
60 hour
F50; ASTM D1693B
ExxonMobil LLDPE LLP 8555.25 Linear Low Density Polyethylene Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
ESCR 10% Igepal® 60 hour
60 hour
ASTM D1693
ExxonMobil LLP8555.24 Rotational Molding Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
ESCR 10% Igepal® 60 hour
60 hour
ASTM D1693
ExxonMobil LLP8555.25 Rotational Molding Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
ESCR 10% Igepal® 60 hour

@Thickness 2.00 mm,
Temperature 50.0 °C
60 hour

@Thickness 0.0787 in,
Temperature 122 °F
0.3 mm notched-plaques; ASTM-D1693
Braskem BS002HS HDPE Blow Molding Polyethylene Copolymer
Resin BS002HS is a high-density polyethylene, bimodal copolymer. It presents good rigidity, good impact resistance, and good reproducibility of the weight of the bottles. It also has excellent envir..