Physical Properties | Metric | English | Comments |
---|---|---|---|
Storage Temperature | <= 25.0 °C | <= 77.0 °F | |
Gwent Electronic Materials C2000808D2 Silver Backlight Ink Silver Ink C2000808D2 is a high resistance ink designed for use as the heating bars and tracks on automobile backlights and other circuits on glass. It has dark color when printed and fired on floa.. |
|||
Storage Temperature | <= 25.0 °C | <= 77.0 °F | cool dry place |
Gwent Electronic Materials R2040212D3 High Viscosity Acrylic Pressure Adhesive for Diagnostic Sensors This material has a high viscosity, it is a water based acrylic pressure sensitive screen printable adhesive. It can be used in many different diagnostic applications such as test cards, assays and.. |
|||
Storage Temperature | 25.0 °C | 77.0 °F | |
Henkel Hysol EA 9330.3 Paste Adhesive System Non-slump, thixotropic adhesive with high peel strength and excellent environmental durability.Applications:Structural Repair Composite Bonding |
|||
Storage Temperature | 25.0 °C | 77.0 °F | |
Henkel Hysol EA 9203 Primer Primer enhances adhesion on poorly prepared surfaces. Requires only room temperature drying prior to bond. Use with room-temperature-curing paste adhesives.Applications: Sprayable Metal and Honeyco.. |
|||
Storage Temperature | 25.0 °C | 77.0 °F | |
Henkel Hysol EA 9309.3NA Paste Adhesive System Toughened adhesive with excellent peel strength. Contains glass beads for bond line control.Applications: Structural Repair Composite Bonding |
|||
Storage Temperature | 25.0 °C | 77.0 °F | |
Henkel Hysol EA 9359.3 Paste Adhesive System Excellent peel and shear strength. Bonds a variety of substrates.Applications: Structural Repair Composite Bonding |
|||
Storage Temperature | 25.0 °C | 77.0 °F | |
Henkel Hysol EA 9360 Paste Adhesive System Structural adhesive, exhibits excellent peel strength, tensile lap shear strength.Applications: Structural Repair Composite Bonding Liquid Shim |
|||
Storage Temperature | <= 25.0 °C | <= 77.0 °F | |
Silon Tabond 2002 Adhesive Resin TABOND 2002 is ethylene-octene Plastomer / LLDPE modified with maleic anhydride functional groups which promote bonding with different materials like polar polymers, metals and surface treated glass.. |
|||
Storage Temperature | <= 25.0 °C | <= 77.0 °F | |
Silon Taboradd 13-08480 Processing Aid Masterbatch High concentrated Masterbatch with a highly effective processing aid especially for polyethylene, but also for most polyolefine.Information provided by Silon |
|||
Storage Temperature | <= 25.0 °C | <= 77.0 °F | |
Silon Taboradd 23-08450 Processing Aid Masterbatch Masterbatch with a highly effective processing aid for polyolefin.Information provided by Silon |
|||
Storage Temperature | <= 25.0 °C | <= 77.0 °F | |
Silon Taborex TA 2111 HD Catalyst Masterbatch Masterbatch for the use with SILON Silane crosslinkable PE-Xb Compounds TA 1108 HD, TA 1109 HD. TA 2111 HD contains the cross-linking catalyst to complete together with the above-mentioned graft a S.. |
|||
Storage Temperature | <= 25.0 °C | <= 77.0 °F | |
Silon Taborex TA 2120 HD Catalyst Masterbatch Masterbatch for the use with SILON Silane crosslinkable PE-Xb Compounds TA 1104 HD, TA 1105 HD, TA 1116 HD. TA 2120 HD contains the cross-linking catalyst to complete together with the above-mention.. |
|||
Storage Temperature | <= 25.0 °C | <= 77.0 °F | |
Silon Taborex TA 2121 HD Catalyst Masterbatch Masterbatch for the use with SILON Silane crosslinkable PE-Xb Compounds TA 1105 HD, TA 1109 HD and TA 1117 HD. TA 2121 HD contains the cross-linking catalyst to complete together with the above-ment.. |
|||
Storage Temperature | <= 25.0 °C | <= 77.0 °F | |
Silon Taborex TA 2126 HD Catalyst Masterbatch Masterbatch for the use with SILON Silane cross-linkable PE-Xb Compounds TA 1108 HD, TA 1109 HD. TA 2126 HD contains the cross-linking catalyst to complete together with the above-mentioned graft a .. |
|||
Storage Temperature | <= 25.0 °C | <= 77.0 °F | |
Silon Taborex TA 2143 HD Catalyst Masterbatch Masterbatch for the use with SILON PE-Xb Compounds TA 1108 HD, TA 1132 HD and TA 1134 HD. TABOREX TA 2143 HD contains a cross-linking catalyst and a part of the long term stabilising system for the .. |
|||
Storage Temperature | <= 25.0 °C | <= 77.0 °F | |
Silon Taborex TA 2343 HD Catalyst Masterbatch Masterbatch for the use with SILON Silane crosslinkable PE-Xb Compounds TA 1108 HD, TA 1116 HD and TA 1117 HD. TA 2343 HD contains the cross-linking catalyst to complete together with the above-ment.. |
|||
Storage Temperature | <= 25.0 °C | <= 77.0 °F | |
Silon Taborex TA 2359 HD Catalyst Masterbatch Masterbatch for the use with SILON Silane crosslinkable PE-Xb Compounds TA 3001 HD. TA 2359 HD contains the cross-linking catalyst to complete together with the above-mentioned graft a Sioplas Syste.. |
|||
Storage Temperature | <= 25.0 °C | <= 77.0 °F | |
Akzo Nobel Trigonox® C-50D-pd Peroxide Cure Agent Trigonox C-50D-pd is a monofunctional peroxide which is used for the crosslinking of polyolefins as well as natural rubber and synthetic rubbers. Chemical Description: tert-Butyl peroxybenzoate, pow.. |
|||
Storage Temperature | <= 25.0 °C | <= 77.0 °F | |
Akzo Nobel Trigonox® ESP Peroxide Cure Agent Trigonox ESP is a peroxide formulation for the curing of unsaturated polyester resins in the presence of a cobalt accelerator.Chemical Description: Methyl isobutyl ketone peroxide and cyclohexanone .. |
|||
Storage Temperature | <= 25.0 °C | <= 77.0 °F | |
Akzo Nobel Trigonox® HM Peroxide Cure Agent Trigonox HM is a peroxide formulation for the curing of unsaturated polyester resins as such or in the presence of a cobalt accelerator.Chemical Description: Methyl isobutyl ketone peroxide, 45% sol.. |
|||
Storage Temperature | <= 25.0 °C | <= 77.0 °F | |
Akzo Nobel Trigonox® C-40B-pd Peroxide Cure Agent Trigonox C-40B-pd is a monofunctional peroxide which is used for the crosslinking of organic rubbers and silicone rubbers.Chemical Description: tert-Butyl peroxybenzoate, powder, 40% with inert fill.. |
|||
Storage Temperature | 25.0 °C | 77.0 °F | |
Henkel Hysol EA 9320NA Paste Adhesive System High shear and high peel adhesive system with room temperature cure. |
|||
Storage Temperature | 25.0 °C | 77.0 °F | |
Henkel Hysol EA 9330 Paste Adhesive System Easy mix adhesive with high peel strength and excellent environmental durability.Applications: Structural Repair Composite Bonding |
|||
Storage Temperature | 25.0 °C | 77.0 °F | |
Henkel Hysol EA 9394.2 Paste Adhesive System Fast cure adhesive for liquid shim and potting. Handling strength within 6 - 8 hours.Applications: Potting Structural Repair Liquid Shim |
|||
Storage Temperature | 25.0 °C | 77.0 °F | |
Gwent Electronic Materials C2010809D3 Silver Ink Silver Ink C2010809D3 is designed for printing via, when screen printed onto LTCC tape. It is compatible with other members of the GEM range of Silver LTCC Inks and most LTCC tape systems on the ma.. |
|||
Storage Temperature | 25.0 °C | 77.0 °F | |
Gwent Electronic Materials C2030304D2 Aluminum Ink C2030304D2 is designed as a screen printing ink for termination of Barium Titanate based PTC devices.This Ink is in a ready to use form at a viscosity suitable for automatic or semiautomatic screen .. |
|||
Storage Temperature | 25.0 °C | 77.0 °F | |
Henkel Hysol EA 9394/C-2 Paste Adhesive System Elevated cure, thixotropic adhesive with structural properties to 450°F / 232°C.Application: Structural Repair |
|||
Storage Temperature | 25.0 °C | 77.0 °F | |
Henkel Hysol EA 9396 Paste Adhesive System Two-part, low viscosity, unfilled version of Hysol EA 9394. Qualified to BMS 8-301.Applications: Structural Repair Low Viscosity Wet Lay-Up Composite Bonding |
|||
Storage Temperature | 25.0 °C | 77.0 °F | |
Henkel Hysol EA 9396/C-2 Paste Adhesive System Two-part, elevated cure, unfilled, low viscosity adhesive with structural properties to 400°F / 204°C.Applications: Structural Repair Low Viscosity Wet Lay-Up Composite Bonding |
|||
Storage Temperature | 25.0 °C | 77.0 °F | |
Henkel Hysol EA 960F Paste Adhesive System Fast-set fairing and smoothing compound for exterior aircraft surfaces.Sandable after 6 hours |