Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.02 g/cc @Temperature 25.0 °C |
0.0368 lb/in³ @Temperature 77.0 °F |
|
BASF Pluracol® 1603 Molded Foam Polyol Description: Pluracol® 1603 polyol is a primary hydroxyl terminated polyether polyol containing an LVI inhibitor package making it ideal for molded seating foam applications. It has an actual funct.. |
|||
Density | 1.02 g/cc @Temperature 25.0 °C |
0.0368 lb/in³ @Temperature 77.0 °F |
|
BASF Pluracol® 2086 Slabstock Foam Polyol Description: Pluracol® 2086 polyol is a nominal 2800 molecular weight polyether triol capable of producing a broad range of flexible slabstock polyurethane foams.Information provided by BASF |
|||
Density | 1.02 g/cc @Temperature 25.0 °C |
0.0368 lb/in³ @Temperature 77.0 °F |
|
BASF Pluracol® 2100 Slabstock HR Foam Polyol Description: Pluracol® 2100 polyol is a primary terminated conventional triol designed to be used in combination with Pluracol 2130 for the production of a broad range of slabstock HR foams. Plurac.. |
|||
Density | 1.02 g/cc @Temperature 37.8 °C |
0.0368 lb/in³ @Temperature 100 °F |
|
BASF Pluracol® 355 Specialty Polyol Description: Pluracol® 355 polyol is an amine-based tetrol of low equivalent weight with built-in catalytic activity. Because of its unusual behavior, this polyol has found wide application in flex.. |
|||
Density | 1.02 g/cc @Temperature 25.0 °C |
0.0368 lb/in³ @Temperature 77.0 °F |
|
BASF Pluracol® 380 Specialty Polyol Description: Pluracol® 380 polyol is a high molecular weight, primary hydroxyl terminated triol. The combination of high molecular weight and reactivity makes Pluracol 380 useful in the preparation.. |
|||
Density | 1.02 g/cc @Temperature 25.0 °C |
0.0368 lb/in³ @Temperature 77.0 °F |
|
BASF Pluracol® 816 Molded Foam Polyol Description: Pluracol® 816 polyol is a high molecular weight triol which was developed for use in high resiliency molded foam formulations. Used in combination with graft polyols, such as Pluracol .. |
|||
Density | 1.02 g/cc @Temperature 60.0 °C |
0.0368 lb/in³ @Temperature 140 °F |
|
BASF Pluracol® P2010 Specialty Polyol Description: Pluracol® P polyols are a series of five polypropylene glycols formed by adding propylene oxide to a propylene glycol nucleus. Pluracol P1010, P2010 and 1044 (formerly P4010) are used .. |
|||
Density | 1.02 g/cc @Temperature 25.0 °C |
0.0368 lb/in³ @Temperature 77.0 °F |
|
BASF Pluracol® TP 740 Specialty Polyol Description: Pluracol® TP polyols are a series of four tri-functional polyols formed by adding propylene oxide to a trimethylol propane nucleus. All Pluracol TP polyols are used in flexible and rig.. |
|||
Density | 1.02 g/cc @Temperature 25.0 °C |
0.0368 lb/in³ @Temperature 77.0 °F |
|
BASF Pluracol® 1528 FF Molded Foam Polyol Description: Pluracol® 1528FF polyol is a graft polyol based on a high reactivity polyether triol containing approximately 45% acrylonitrile/styrene copolymer. Pluracol 1528FF is a "fine-filtered" .. |
|||
Density | 1.02 g/cc @Temperature 25.0 °C |
0.0368 lb/in³ @Temperature 77.0 °F |
|
BASF Pluracol® 2090 Specialty Polyol Description: Pluracol® 2090 polyol is a high molecular weight, primary hydroxyl terminated triol. The combination of high molecular weight and reactivity makes Pluracol 2090 useful in the preparati.. |
|||
Density | 1.02 g/cc @Temperature 25.0 °C |
0.0368 lb/in³ @Temperature 77.0 °F |
|
BASF Pluracol® 4156 Slabstock Foam Polyol Description: Pluracol® 4156 polyol is a 56 hydroxyl number (nominal 3000 molecular weight) polyether triol capable of producing a broad range of flexible slabstock polyurethane foams for furniture,.. |
|||
Density | 1.02 g/cc @Temperature 37.8 °C |
0.0368 lb/in³ @Temperature 100 °F |
|
BASF Pluracol® 628 Specialty Polyol Description: Pluracol® 628 polyol is a high molecular weight, primary hydroxyl terminated diol used in the manufacture of polyurethane shoe soles and fascia products. Pluracol 628 can also be used .. |
|||
Density | 1.02 g/cc @Temperature 48.9 °C |
0.0368 lb/in³ @Temperature 120 °F |
|
BASF Pluracol® GP 730 Specialty Polyol Description: Pluracol® GP polyols are a series of four trifunctional polyols formed by adding propylene oxide to a glycerine nucleus. All Pluracol GP polyols are used in the preparation of polyure.. |
|||
Density | 1.02 g/cc @Temperature 37.8 °C |
0.0368 lb/in³ @Temperature 100 °F |
|
BASF Pluracol® TP 440 Specialty Polyol Description: Pluracol® TP polyols are a series of four tri-functional polyols formed by adding propylene oxide to a trimethylol propane nucleus. All Pluracol TP polyols are used in flexible and rig.. |
|||
Density | 1.02 g/cc @Temperature 40.0 °C |
0.0368 lb/in³ @Temperature 104 °F |
|
BASF Quadrol® Specialty Polyol Description: Quadrol® polyol is N, N, N´, N´-Tetrakis (2-hydroxypropyl) ethylene-diamine. Quadrol has proven to be an excellent cross-linking agent and catalyst for use in polyurethane coatings a.. |
|||
Density | 1.02 g/cc @Temperature 25.0 °C |
0.0368 lb/in³ @Temperature 77.0 °F |
|
BASF Pluracol® 945 Molded Foam Polyol Description: Pluracol® 945 polyol is a high molecular weight polyol for use in high water, low-density automotive seating foams where a high degree of foam stability is required. In combination wit.. |
|||
Density | 1.02 g/cc @Temperature 25.0 °C |
0.0368 lb/in³ @Temperature 77.0 °F |
Part B; ASTM D1622 |
Hexcel® Redux® 810 Two-Part Epoxy Paste Adhesive Redux® 810 is a multi-purpose, high shear and peel strength, two-part, toughened epoxy paste adhesive with corrosion-inhibiting properties.Features: Available in cartridges with a static mixer and .. |
|||
Density | 1.02 g/cc @Temperature 25.0 °C |
0.0368 lb/in³ @Temperature 77.0 °F |
|
BASF Pluracol® 1421 Molded Foam Polyol Description: Pluracol® 1421 polyol is a high molecular weight triol which was developed for use in high resiliency molded foam formulations. Used in combination with graft polyols, such as Pluracol.. |