Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0077 cm/cm @Time 86400 sec |
0.0077 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Lubricomp GL004 PSU (Asia Pacific) LNP* Lubricomp* GL004 is a compound based on Polysulfone resin containing PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia Pacifi.. |
|||
Linear Mold Shrinkage, Flow | 0.0077 cm/cm @Time 86400 sec |
0.0077 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Stat-loy A3000Z ABS LNP* Stat-loy* A3000Z is a compound based on Acrylonitrile Butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for t.. |
|||
Linear Mold Shrinkage, Flow | 0.0077 cm/cm @Time 86400 sec |
0.0077 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Stat-loy A3000Z ABS (Asia Pacific) LNP* Stat-loy* A3000Z is a compound based on Acrylonitrile Butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for t.. |
|||
Linear Mold Shrinkage, Flow | 0.0077 cm/cm @Time 86400 sec |
0.0077 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP RF002ES PA 66 LNP THERMOCOMP* RF002ES is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized. |
|||
Linear Mold Shrinkage, Flow | 0.0077 cm/cm @Time 86400 sec |
0.0077 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON DD0009PC PC LNP STAT-KON* DD0009PC is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Linear Mold Shrinkage, Flow | 0.0077 cm/cm @Time 86400 sec |
0.0077 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Lubricomp GL004 PSU LNP* Lubricomp* GL004 is a compound based on Polysulfone resin containing PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Americas re.. |