Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.012 cm/cm

@Time 86400 sec
0.012 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP KF002 Acetal Copolymer
LNP THERMOCOMP* KF002 is a compound based on Acetal Copolymer resin containing 10% Glass Fiber.
Linear Mold Shrinkage, Flow 0.012 cm/cm

@Time 86400 sec
0.012 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Thermocomp KF003 Acetal Copoly
LNP* Thermocomp* KF003 is a compound based on Acetal Copolymer resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Linear Mold Shrinkage, Flow 0.012 cm/cm

@Time 86400 sec
0.012 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Thermocomp KF003 Acetal Copoly (Asia Pacific)
LNP* Thermocomp* KF003 is a compound based on Acetal Copolymer resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
Linear Mold Shrinkage, Flow 0.012 cm/cm

@Time 86400 sec
0.012 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP KX97390 Acetal Copolymer
LNP THERMOCOMP* KX97390 is a compound based on Acetal Copolymer resin containing Glass Fiber. Added features of this material include: Chemically Coupled.
Linear Mold Shrinkage, Flow 0.012 cm/cm

@Time 86400 sec
0.012 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP MB006S PP
LNP THERMOCOMP* MB006S is a compound based on Polypropylene resin containing 30% Glass Bead. Added features of this material include: Heat Stabilized.
Linear Mold Shrinkage, Flow 0.012 cm/cm

@Time 86400 sec
0.012 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP PH0460A PA 6
LNP* THERMOCOMP* PH0460A is a compound based on Nylon 6. Added feature of this material is: High Specific Gravity.
Linear Mold Shrinkage, Flow 0.012 cm/cm

@Time 86400 sec
0.012 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP TH0300A PUR
LNP THERMOCOMP* TH0300A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity.
Linear Mold Shrinkage, Flow 0.012 cm/cm

@Time 86400 sec
0.012 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP TH0300A PUR
LNP THERMOCOMP* TH0300A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity.
Linear Mold Shrinkage, Flow 0.012 cm/cm

@Time 86400 sec
0.012 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP TH0300A PUR (Asia Pacific)
LNP THERMOCOMP* TH0300A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity.
Linear Mold Shrinkage, Flow 0.012 cm/cm

@Time 86400 sec
0.012 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP TH0300A PUR (Asia Pacific)
LNP THERMOCOMP* TH0300A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity.
Linear Mold Shrinkage, Flow 0.012 cm/cm

@Time 86400 sec
0.012 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP KF002XXP Acetal Copoly
LNP* Thermocomp* KF002XXP is a compound based on Acetal Copolymer resin containing 10% Glass Fiber. Added features of this material include: Chemically Coupled.
Linear Mold Shrinkage, Flow 0.012 - 0.014 cm/cm

@Time 86400 sec
0.012 - 0.014 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP MB008S PP
LNP* THERMOCOMP* MB008S is a compound based on Polypropylene resin containing 40% Glass Bead. Added features of this material include: Heat Stabilized.
Linear Mold Shrinkage, Flow 0.012 - 0.014 cm/cm

@Time 86400 sec
0.012 - 0.014 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Thermocomp MB008S PP (Asia Pacific)
LNP* Thermocomp* MB008S is a compound based on Polypropylene resin containing Glass Bead. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia Pa..
Linear Mold Shrinkage, Flow 0.012 cm/cm

@Time 86400 sec
0.012 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOTUF MF004AI PP
LNP* Thermotuf* MF004AI is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: High Impact.
Linear Mold Shrinkage, Flow 0.012 cm/cm

@Time 86400 sec
0.012 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOTUF MF004AI PP (Asia Pacific)
LNP* Thermotuf* MF004AI is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: High Impact.
Linear Mold Shrinkage, Flow 0.012 cm/cm

@Time 86400 sec
0.012 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP PH0460A PA 6 (Asia Pacific)
LNP* Thermocomp* PH0460A is a compound based on Nylon 6 resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.
Linear Mold Shrinkage, Flow 0.012 cm/cm

@Time 86400 sec
0.012 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON MFD02 PP
LNP* STAT-KON* MFD02 is a compound based on Polypropylene resin containing 10% Glass Fiber. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Flow 0.012 cm/cm

@Time 86400 sec
0.012 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON MFD02 PP (Asia Pacific)
LNP* Stat-kon* MFD02 is a compound based on Polypropylene resin containing Glass Fiber, Carbon Powder. Added features of this material include: Electrically Conductive.