Polymer Property : Linear Mold Shrinkage, Flow = 0.024 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.021 - 0.024 cm/cm

@Time 86400 sec
0.021 - 0.024 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP WL004 PBT
LNP LUBRICOMP* WL004 is a compound based on PBT resin containing 20% PTFE. Added features of this material include: Wear Resistant.
Linear Mold Shrinkage, Flow 0.020 - 0.024 cm/cm

@Time 86400 sec
0.020 - 0.024 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Stat-loy K3000 Acetal Copoly
LNP* Stat-loy* K3000 is a compound based on Acetal Copolymer resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Americas regi..
Linear Mold Shrinkage, Flow 0.020 - 0.024 cm/cm

@Time 86400 sec
0.020 - 0.024 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Stat-loy K3000 Acetal Copoly
LNP* Stat-loy* K3000 is a compound based on Acetal Copolymer resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Americas regi..
Linear Mold Shrinkage, Flow 0.020 - 0.024 cm/cm

@Time 86400 sec
0.020 - 0.024 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Stat-loy K3000 Acetal Copoly (Asia Pacific)
LNP* Stat-loy* K3000 is a compound based on Acetal Copolymer resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Asia Pacific ..
Linear Mold Shrinkage, Flow 0.020 - 0.024 cm/cm

@Time 86400 sec
0.020 - 0.024 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Stat-loy K3000 Acetal Copoly (Asia Pacific)
LNP* Stat-loy* K3000 is a compound based on Acetal Copolymer resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Asia Pacific ..