Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K Factor (ISO) | 6400 µm/km | 6400 µm/km | |
Quadrant EPP Quadrant LSG PSU extruded (ISO Data) Within its portfolio of Life Science Grade Engineering Plastic Products - specifically developed for applications in the medical, pharmaceutical and biotechnology industries - Quadrant offers QUADRA.. |
|||
K Factor (ISO) | 6400 µm/km | 6400 µm/km | |
Quadrant EPP Quadrant PSU unfilled, extruded (ISO Data) Quadrant 1000 PSU is a slightly yellow, translucent (non-optical quality) amorphous thermoplastic material, offering a combination of excellent mechanical, thermal and electrical properties. It ofte.. |