Polymer Property : Tensile Impact = 107 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Impact >= 107 J/cm
>= 200 ft-lb/in
ASTM D1822
LyondellBasell Petrothene® LP5100 High Density Polyethylene
ApplicationsPETROTHENE LP 5100 is especially designed for large-part blow molding of durable goods and deep-draw sheet extrusion/thermoforming applications. LP 5100 exhibits excellent impact resist..
Tensile Impact 107 J/cm
200 ft-lb/in
Filling Breaking Strength
Hexcel® HexForce™ 1526 Fiber Glass Fabric
Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential ..
Tensile Impact 107 J/cm
200 ft-lb/in
Warp Breaking Strength
Hexcel® HexForce™ 1692 Fiber Glass Fabric
Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential ..
Tensile Impact 107 J/cm
200 ft-lb/in
Warp Breaking Strength
Hexcel® HexForce™ 2116 Fiber Glass Fabric
Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential ..
Tensile Impact 107 J/cm
200 ft-lb/in
Filling Breaking Strength
Hexcel® HexForce™ 4180 Fiber Glass Fabric
Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential ..
Tensile Impact 107 J/cm
200 ft-lb/in
Warp Breaking Strength
Hexcel® HexForce™ 7579 Fiber Glass Fabric
Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential ..
Tensile Impact 107 J/cm
200 ft-lb/in
Filling Breaking Strength
Hexcel® HexForce™ 7580 Fiber Glass Fabric
Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential ..
Tensile Impact 107 J/cm
200 ft-lb/in
Filling Breaking Strength
Hexcel® HexForce™ 1528 Fiber Glass Fabric
Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential ..
Tensile Impact 107 J/cm
200 ft-lb/in
Warp Breaking Strength
Hexcel® HexForce™ 1579 Fiber Glass Fabric
Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential ..
Tensile Impact 107 J/cm
200 ft-lb/in
Warp Breaking Strength
Hexcel® HexForce™ 220 Fiber Glass Fabric
Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential ..