Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact | 240 J/cm | 450 ft-lb/in | Filling Breaking Strength |
Hexcel® HexForce™ 1564 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Tensile Impact | 240 J/cm | 450 ft-lb/in | Warp Breaking Strength |
Hexcel® HexForce™ 1581 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Tensile Impact | 240 J/cm | 450 ft-lb/in | Filling Breaking Strength |
Hexcel® HexForce™ 332 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Tensile Impact | 240 J/cm | 450 ft-lb/in | Filling Breaking Strength |
Hexcel® HexForce™ 6781 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Tensile Impact | 240 J/cm | 450 ft-lb/in | Filling Breaking Strength |
Hexcel® HexForce™ 7781 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Tensile Impact | 240 J/cm | 450 ft-lb/in | Filling Breaking Strength |
Hexcel® HexForce™ 8800 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Tensile Impact | 240 J/cm | 450 ft-lb/in | Filling Breaking Strength |
Hexcel® HexForce™ 232 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Tensile Impact | 240 J/cm | 450 ft-lb/in | Filling Breaking Strength |
Hexcel® HexForce™ 7587 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |