Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 1.48 MPa | 215 psi | |
Parker Chomerics Tecknit Teckfip™ FIP-X Formed in Place Conductive Elastomer Description: FIP-X is Tecknit’s newest compound and features a conductive powder that is a unique particle combining tungsten carbide and aluminum. The premium advantage of this compound is its ab.. |