Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | >= 10.3 MPa | >= 1490 psi | ASTM D412 |
S&E Specialty Polymers G-04-036ESD PVC Application: High Performance, PVC based compound with antistatic properties. G-04-036ESD is suitable for Gamma radiation sterilization.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | 10.3 MPa | 1490 psi | ASTM D638 |
S&E Specialty Polymers GTPO8280 NATURAL PVC Application: EPDM Based flexible polyolefin compound.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | 10.3 MPa | 1500 psi | ASTM D638 |
Quadrant EPP Fluorosint® 207 PTFE, Compression Molded Synthetic Mica-filled PTFE (ASTM Product Data Sheet) |
|||
Tensile Strength | 10.3 MPa | 1500 psi | |
Parker Chomerics CHO-SHRINK® Tubing Conductive Heat Shrinkable EMI Shielding Description: CHO-SHRINK tubing is a heat shrinkable polyolefin manufactured to MIL-R-46846 Type 5, modified to provide effective 360° EMI shielding for cables. CHO-SHRINK tubing offers significant .. |
|||
Tensile Strength | 10.3 MPa @Strain 100 % |
1490 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible A8504 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 10.3 MPa @Strain 100 % |
1490 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible B85UB Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 10.3 MPa @Strain 100 % |
1490 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible B90T0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 10.3 MPa @Strain 100 % |
1490 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible XV3875 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
Tensile Strength | 10.3 MPa @Strain 100 % |
1490 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible G8024 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 10.3 MPa | 1500 psi | across grain; ASTM F152 |
Garlock 2900 Compressed Aramid Fiber Gasketing, Nitrile Binder Aramid fibers with a nitrile binder.Ideal for utility servicesExcellent sealabilityImproved thermal stabilityGood for general serviceMedia: Water, aliphatic hydrocarbons, oils, gasolineInformation .. |
|||
Tensile Strength | >= 10.3 MPa | >= 1500 psi | |
Garlock 509 Butyl Sheet Rubber Style #509 is a branded, chloro-butyl sheet rubber product.Information provided by Garlock Rubber Technologies |
|||
Tensile Strength | >= 10.3 MPa | >= 1500 psi | |
Garlock 5260 Neoprene Sheet Rubber This blended neoprene sheet is used where good oil, petroleum, ozone and weathering-resistance is needed.Black, smooth finishInformation provided by Garlock Rubber Technologies |
|||
Tensile Strength | >= 10.3 MPa | >= 1500 psi | |
Garlock 5360 Nitrile Sheet Rubber Nitrile sheet is primarily used for applications where resistance to oil, solvents and fuels is required.Style #5360 is a medium-hard, premium-grade nitrile sheet, also available in 40, 50, 70 and 8.. |
|||
Tensile Strength | 10.3 MPa | 1500 psi | across grain; ASTM F152 |
Garlock 5507 Compressed Inorganic Fiber Gasketing, EPDM Binder Inorganic fibers with an EPDM binder.Inorganic fiber gasketing offers excellent thermal stability with minimal weight lossReduced creep relaxation and improved torque retention provide optimal seala.. |
|||
Tensile Strength | >= 10.3 MPa | >= 1500 psi | |
Garlock 7797 Neoprene Sheet Rubber This blended neoprene sheet is used where good oil, petroleum, ozone and weathering-resistance is needed.Black, smooth cloth finishInformation provided by Garlock Rubber Technologies |
|||
Tensile Strength | 10.3 MPa | 1500 psi | ASTM D412 |
Garlock 7992 Neoprene Rubber Diaphragm, Fabric Insert Neoprene rubber with 22oz. hose duck fabric insertCombines elasticity and extensibility of rubber with strength of fabric insert. Specially compounded in varying burst strengths for almost any serv.. |
|||
Tensile Strength | >= 10.3 MPa | >= 1500 psi | |
Garlock SBR Extruded Skirtboard SBR rubber extruded skirtboard for protection applicationsInformation provided by Garlock Rubber Technologies |
|||
Tensile Strength | 10.3 MPa | 1490 psi | Measured on extrusion cast film; ASTM D412 |
Kraton® G1645 M (SEBS) Linear Triblock Copolymer Description: Kraton G1645 M is a linear triblock copolymer based on styrene and ethylene/butylene. It is supplied from North America in the physical form identified: Kraton G1645 MO - supplied as a .. |
|||
Tensile Strength | 10.3 MPa | 1490 psi | |
Momentive Performance Materials TSE 2267 Heat Cured Rubber - High Duro Translucent Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tensile Strength | 10.3 MPa | 1500 psi | across grain; ASTM F152 |
Garlock 9800 Compressed Carbon Fiber Gasketing, SBR Binder Carbon fibers with a SBR binder.Carbon fiber gasketing excels in harshest conditions- intense heat, high pressure, saturated steam and hot oilsLaboratory tested for fire safetyMaintains effective se.. |
|||
Tensile Strength | 10.3 MPa | 1500 psi | ASTM D152 |
Thermoseal soft-chem® PTFE Gasketing Thermoseal® soft-chem® expanded PTFE sealing material provides excellent corrosion resistance and impermeability along with superior creep resistance and sealability for use in all types of applic.. |
|||
Tensile Strength | 10.3 MPa | 1500 psi | Silicone Property; ASTM D412 |
Arlon HS930-10R##-P4 0.030" (0.762 mm) Self-Fusing Silicone Tape (Rectangular, Unsupported) Description: High Strength, 1 inch wide, 30 mil thick, Red, Rectangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicat.. |
|||
Tensile Strength | 10.3 MPa | 1500 psi | |
AlphaGary Garathane™ X 05-309 A3 Polyurethane based compound Abrasion & Slip Resistant |
|||
Tensile Strength | 10.3 MPa | 1500 psi | |
AlphaGary PVC 2215/3X-55 Black 1000 Polyvinyl Chloride Thermoplastic Molding grade for grommets and connectors with fungus resistance |
|||
Tensile Strength | 10.3 MPa | 1500 psi | Adhesion |
Atom Adhesives AA-DUCT 905 Epoxy Adhesive AA-DUCT 905 is a single component epoxy, formulated with pure silver powder combined with organic binders and solvents to produce electrically conductive paths, films or patterns over non-conductive.. |
|||
Tensile Strength | 10.3 MPa | 1500 psi | |
Teknor Apex Elexar® EL 1934A Thermoplastic Elastomer Notes: Elexar® is a family of styrene block copolymer thermoplastic elastomers, often referred to as thermoplastic rubber (TPR). Elexar® "rubber-like" compounds offer superior electrical properti.. |
|||
Tensile Strength | 10.3 MPa | 1500 psi | |
AlphaGary PVC 7731 Polyvinyl Chloride Thermoplastic Automotive Molding |
|||
Tensile Strength | 10.3 MPa | 1500 psi | |
AlphaGary PVC GM 5065 Natural Polyvinyl Chloride Thermoplastic A 105°C rated, lead & cadmium free, UL-94 V2 molding compound |
|||
Tensile Strength | 10.3 MPa | 1500 psi | |
AlphaGary PVC GM 5075 Polyvinyl Chloride Thermoplastic A 105°C rated, lead & cadmium free, UL-94 V2 molding compound |