Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 72.4 MPa | 10500 psi | ASTM D-638 |
Plaskolite Optix® CP - 86 General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Tensile Strength | 72.4 MPa | 10500 psi | ASTM D-638 |
Plaskolite West Optix® CP - 86 General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Tensile Strength | 72.4 MPa | 10500 psi | ASTM D638 |
Quadrant EPP Ertalyte® TX Internally Lubricated Semi-Crystalline Polyester (ASTM Product Data Sheet) |
|||
Tensile Strength | 72.4 MPa | 10500 psi | ASTM D638 |
Quadrant EPP Nylatron® WP PA (ASTM Product Data Sheet) |
|||
Tensile Strength | 72.4 MPa | 10500 psi | ASTM D638 |
Quadrant EPP Quadrant Nylon 612 |
|||
Tensile Strength | 72.4 MPa | 10500 psi | ASTM D-638 |
Plaskolite West Optix® CP - 86 UVA General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Tensile Strength | 72.4 MPa | 10500 psi | ASTM D638 |
Quadrant EPP Quadrant 1000 LSP PC Extruded Unfilled Polycarbonate |
|||
Tensile Strength | 72.4 MPa | 10500 psi | ASTM D638 |
Quadrant EPP Quadrant PC 1000 Extruded, Unfilled, Polycarbonate (ASTM Product Data Sheet) |
|||
Tensile Strength | 72.4 MPa | 10500 psi | ASTM D638 |
Quadrant EPP Semitron® CMP LL5 Polyester (ASTM Product Data Sheet) Enhanced semi-crystalline polyester product for extended service in CMP retaining rings. Superior performance, especially in oxide processes, and cost effective relative to standard ring materials. .. |
|||
Tensile Strength | 72.4 MPa | 10500 psi | |
Lucite International Elvacite ® 2010 Acrylic Resin Elvacite® 2010 is a medium molecular weight methyl methacrylate polymer. 2010 is excellent for use as a general purpose grade for lacquer coatings, such as barrier topcoats for vinyl. It provides.. |
|||
Tensile Strength | 72.4 MPa | 10500 psi | ASTM D638 |
Solvay Specialty Polymers Radel® R-7535 Polyphenylsulfone (PPSU) Radel® R-7535 polyphenylsulfone resin is a cost-effective solution for aircraft interior applications. This product complies with the FAA regulation 14CFR Part 25 Appendix F, offering vertical bu.. |
|||
Tensile Strength | 72.4 MPa | 10500 psi | ASTM D638 |
Solvay Specialty Polymers Radel® R-7558 Polyphenylsulfone (PPSU) Radel® R-7558 polyphenylsulfone resin is a cost-effective solution for aircraft interior applications. This product complies with the FAA regulation 14CFR Part 25 Appendix F, offering vertical bu.. |
|||
Tensile Strength | 72.4 MPa | 10500 psi | ASTM D638 |
Techmer ES Luriblend® PA6 TSX10 Nylon 6 Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant (10%)Features: Lubricated and Good Wear ResistanceInformation provided by TP Composites, Inc. |
|||
Tensile Strength | 72.4 MPa | 10500 psi | ASTM D638 |
Teknor Apex Chemlon® 182 Nylon 66, Non-Halogenated Notes: General Purpose; U.L. 94 V-O at 0.57 mm; Colorable; Flame Retardant Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex |
|||
Tensile Strength | 72.4 MPa | 10500 psi | ASTM D638 |
Teknor Apex Chemlon® 282 Nylon 6, Non-halogenated Features: Flame Retardant; General Purpose; Halogen-free; U.L. 94 V-O at 0.63 mm; ColorableProcessing Method: Injection Molding Forms: Pellets Additive: Flame RetardantInformation Provided by Teknor.. |
|||
Tensile Strength | 72.4 MPa | 10500 psi | ASTM D-638 |
Plaskolite Optix® CP - 86 UVA General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Tensile Strength | 72.4 MPa | 10500 psi | ASTM D638 |
Quadrant EPP Quadrant LSG PC (ASTM Product Data Sheet) Data provided by Quadrant Engineering Plastic Products. |