Mechanical Properties Metric English Comments
Tensile Strength 75.8 MPa
11000 psi
ASTM D-638
Plaskolite Optix® CA - 87 General Purpose Acrylic Resin
OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli..
Tensile Strength 75.8 MPa
11000 psi
ASTM D-638
Plaskolite West Optix® CA - 87 General Purpose Acrylic Resin
Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av..
Tensile Strength 75.8 MPa
11000 psi
ASTM D638
Quadrant EPP Acetron® POM-H Homopolymer Acetal, Unfilled, Extruded (ASTM Product Data Sheet)
Tensile Strength 75.8 MPa
11000 psi
ASTM D638
Quadrant EPP Duratron® PI D7015G PI Bearing Grade Polyimide (ASTM Product Data Sheet)
Tensile Strength 76.0 MPa
11000 psi
at Yield; ISO 527-1/-2
Quadrant EPP Ertalyte® TX PET + solid lubricant, extruded (ISO Data)
Ertalyte TX is a polyethylene terephthalate compound incorporating a uniformly dispersed solid lubricant. Its specific formulation makes it a premium internally lubricated bearing-grade. Ertalyte TX..
Tensile Strength 75.8 MPa

@Temperature 22.8 °C
11000 psi

@Temperature 73.0 °F
ASTM D638
Quadrant EPP Ketron® HPV PEEK High Pressure Velocity Polyetherether Ketone (ASTM Product Data Sheet)
This bearing grade of extruded Ketron PEEK offers the lowest coefficient of friction and best machinability of all Ketron grades. It is ideal for low wear, high PV parts that require chemical resis..
Tensile Strength 75.8 MPa
11000 psi
ASTM D638
Quadrant EPP Nylatron® GSM Nylon, Cast MoS2 Filled Type 6 (ASTM Product Data Sheet)
Tensile Strength 75.8 MPa
11000 psi
ASTM D638
Quadrant EPP Nylatron® NSM Nylon, Cast Solid Lubricant Filled, Type 6 (ASTM Product Data Sheet)
Tensile Strength 75.8 MPa
11000 psi
ASTM D638
Quadrant EPP Quadrant PPSU LSG PPSU, Extruded, Unfilled, Polyphenylsulfone (ASTM Product Data Sheet)
Tensile Strength 75.8 MPa
11000 psi
ASTM D638
Quantum PPSU
Information provided by Quantum Advanced Engineering Plastics
Tensile Strength 75.8 MPa
11000 psi
ASTM D638
Solvay Specialty Polymers Udel® P-3700 HC Polysulfone (PSU)  (Unverified Data**)
Udel P-3700 HC is a high-clarity grade of polysulfone (PSU) that is nearly water-white in color. This grade was designed to eliminate the yellow cast and provide design flexibility and improved aest..
Tensile Strength 75.8 MPa
11000 psi
ASTM D638
Solvay Specialty Polymers Udel® M-2300 MR Polysulfone (PSU), Mold Release  (discontinued **)
Udel M-2300 MR is an injection-moldable, low-color grade of polysulfone that is nearly water white in color. This material contains a mold release which aids part ejection when parts with low draft ..
Tensile Strength 76.0 MPa

@Temperature 23.0 °C
11000 psi

@Temperature 73.4 °F
DAM; ASTM D638
DuPont Performance Polymers Minlon® 12TA BKB124 Nylon 66  (Unverified Data**)
Minlon® 12TA BKB124 is a 32% mineral reinforced, toughened, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Strength 76.0 MPa
11000 psi
ISO 527
Lucite International Diakon® CLG960 Acrylic Polymer
Information provided by Lucite International
Tensile Strength 75.9 MPa
11000 psi
Henkel Hysol EA 9150 Composite Resin
Low viscosity, toughened system formulated for resin transfer molding. 250°F / 121°C cure and service temperature.Application: Composite Binding
Tensile Strength 75.8 MPa
11000 psi
ASTM D638
Solvay Specialty Polymers Radel® R-7400 Polyphenylsulfone (PPSU)
Radel® R-7300 (for light colors) and R-7400 (for darker colors) polyphenylsulfone resins were developed specifically for aircraft interior applications, and through the use of a proprietary flame..
Tensile Strength 75.8 MPa
11000 psi
ASTM D638
Solvay Specialty Polymers Udel® P-3700 HC Polysulfone (PSU)
Udel® P-3700 HC is a high-clarity grade of polysulfone (PSU) that is nearly water-white in color. This grade was designed to eliminate the yellow cast and provide design flexibility and improved ..
Tensile Strength >= 75.8 MPa

@Temperature 23.9 °C
>= 11000 psi

@Temperature 75.0 °F
Master Bond EP112FLAN-1 Two Component Flexibilized Heat Curing Epoxy
Master Bond EP112FLAN-1 is a toughened two component, high performance epoxy resin system featuring good temperature resistance, high thermal conductivity, fine electrical insulation values and soun..
Tensile Strength >= 75.8 MPa

@Temperature 23.9 °C
>= 11000 psi

@Temperature 75.0 °F
Master Bond EP112FLAO-1 Toughened, Two component, Heat Curing Epoxy
Master Bond EP112FLAO-1 is a toughened two component, high performance epoxy resin system featuring very good temperature resistance, fine thermal conductivity and electrical insulation values with ..
Tensile Strength 75.5 MPa
11000 psi
ASTM D638
E-Polymers TEKAMID® TB120CR Fast Crystallinity PA6 Resin
Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.T-series: Impact modified,..
Tensile Strength 75.8 MPa
11000 psi
ASTM D638
CIP Composites 100 Series Laminated Polymer Bearing Material
The 100 series consists of polyester fabric and one of several solid lubricants (optional) in a resin matrix. Non-metallic, high load, high impact and self lubricating laminated material. Laminated..
Tensile Strength 76.0 MPa

@Strain 15.0 %,
Temperature 0.000 °C
11000 psi

@Strain 15.0 %,
Temperature 32.0 °F
50 mm/min; ISO 527-2
BASF Elastollan R 1000 20% Glass Filled TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan..
Tensile Strength 75.8 MPa
11000 psi
ASTM D638
Aaron Industries AAROPRENE® GFABS 4020 Glass Filled Acrylonitrile-Butadiene Styrene
AAROPRENE® GFABS 4000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified.
Tensile Strength 75.8 MPa
11000 psi
ASTM D638
Solvay Specialty Polymers Radel® R-7300 Polyphenylsulfone (PPSU)
Radel® R-7300 (for light colors) and R-7400 (for darker colors) polyphenylsulfone resins were developed specifically for aircraft interior applications, and through the use of a proprietary flame r..