Mechanical Properties Metric English Comments
Tensile Strength 120 MPa

@Thickness 4.00 mm,
Temperature 23.0 °C
17400 psi

@Thickness 0.157 in,
Temperature 73.4 °F
5.0 mm/min; ISO 527
PolyOne Bergamid™ B70 G30 grey VN7445CF Polyamide 6 (Nylon 6)
Information provided by PolyOne
Tensile Strength 120 MPa
17400 psi
ASTM D638
Solvay Specialty Polymers Amodel® A-1133 NL WH 886 Polyphthalamide (PPA)  (discontinued **)
Amodel A-1133 NL WH 886 resin is a glass reinforced polyphthalamide (PPA ) which is distinguished by its high-reflectivity white color. This grade features a high deflection temperature for compatib..
Tensile Strength 120 - 140 MPa
17400 - 20300 psi
Injection; ISO 527
Raschig Group RESINOL® 87120 EPF Phenolic
Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets ..
Tensile Strength 120 MPa
17400 psi
ASTM D638
Kolon KOCETAL® CF704 Conductive Grade Acetal Resin
Carbon fiber added, high stiffness and conductive grade. Applications: Conductive products. Information provided by API-Kolon.
Tensile Strength 120 MPa
17400 psi
ASTM D638
Kolon KOCETAL® GF105 G/F Reinforced Acetal Resin
Glass fiber reinforced, improved stiffness. Applications: Products for high stiffness, improved fatigue properties. Information provided by API-Kolon.
Tensile Strength 120 MPa
17400 psi
ASTM D638
Solvay Specialty Polymers Veradel® 3320GF Polyethersulfone (PESU), 20% Glass Fiber
Veradel® 3320GF is a 20% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, ..
Tensile Strength >= 120 MPa
>= 17400 psi
IEC 1212-2 5.7
Hippe PF CP 201 Cellulose Paper Reinforced Phenolic Resin - Sheet
Used in mechanical applications. Used in mechanical properties better than other PF CP types. Poor electrical properties under normal humidity. Also available in hot-punching versions.Information..
Tensile Strength >= 120 MPa
>= 17400 psi
IEC 1212-2 5.7
Hippe PF WV 303 Wood veneer Reinforced Phenolic Resin - Sheet
Parallel plied. Used in mechanical applications. Good mechanical properties.Information provided by Hippe.
Tensile Strength >= 120 MPa
>= 17400 psi
IEC 1212-2 5.7
Hippe PF WV 304 Wood veneer Reinforced Phenolic Resin - Sheet
Parallel plied. Used in mechanical and electrical applications.Information provided by Hippe.
Tensile Strength >= 120 MPa
>= 17400 psi
IEC 1212-2 5.7
Hippe UP GM 204 Woven Glass Mat Reinforced Polyester (unsaturated) Resin - Sheet
Used in mechanical and electrical applications. Very high mechanical properties at ambient temperatures. Good mechanical properties at elevated temperatures.Information provided by Hippe.
Tensile Strength >= 120 MPa
>= 17400 psi
IEC 1212-2 5.7
Hippe UP GM 205 Woven Glass Mat Reinforced Polyester (unsaturated) Resin - Sheet
Used in mechanical and electrical applications. Very high mechanical properties at ambient temperatures. Good mechanical properties at elevated temperatures. Flame retardant.Information provided ..
Tensile Strength 120 MPa
17400 psi
dry; ISO 527
Azoty Tarnow™ Tarnamid® T-27 GF15 FRV0 Polyamide 6 - Flame Retarded, Reinforced
Flame retarded grades, flammability class V0, reinforced with 15% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning..
Tensile Strength 120 MPa
17400 psi
dry; ISO 527
Azoty Tarnow™ Tarnamid® T-27 GF15 Polyamide 6 - Glass Fiber Reinforced
15% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High..
Tensile Strength 120 MPa
17400 psi
cond.; ISO 527
Azoty Tarnow™ Tarnamid® T-27 GF35 Polyamide 6 - Glass Fiber Reinforced
35% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High..
Tensile Strength 120 MPa
17400 psi
ASTM D638
Solvay Specialty Polymers Veradel® 3320GF Polyethersulfone (PESU)  (Unverified Data**)
Veradel 3320GF is a 20% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, dime..
Tensile Strength 120 MPa
17400 psi
5 mm/min; ISO 527-1
Sax Polymers SAXAMID 236F6Q32 Nylon 6.6, 30% Glass Fiber
SAXAMID 236F6Q32 is a impact-modified polyamide 6.6 injection-molding-grade reinforced with 30% glass fibers and very good flow properties. It is suitable for applications requiring toughness in com..