Polymer Property : Tensile Strength = 12000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 82.7 MPa
12000 psi
ASTM D638
Quadrant EPP Nylatron® MC® 901 Blue, Heat Stabilized, Type 6 (ASTM Product Data Sheet)
Data provided by Quadrant Engineering Plastic ProductsBroadest size range availabilityGood mechanical and electrical propertiesIdeal balance of strength and toughnessCast as finished parts and near ..
Tensile Strength 82.7 MPa
12000 psi
ASTM D638
Quadrant EPP Quadrant Nylon 101 Extruded, Unfilled, Type 66 Natural and Black (ASTM Product Data Sheet)
Tensile Strength 83.0 MPa
12000 psi
at Yield; ISO 527-1/-2
Quadrant EPP Quadrant PPSU unfilled, extruded (ISO Data)
Quadrant PPSU is a black, amorphous high performance thermoplastic, offering better impact strength and chemical resistance than polysulfone and polyetherimide. Quadrant PPSU also has superior hydro..
Tensile Strength 82.7 MPa
12000 psi
ASTM D638
Quadrant EPP Semitron® ESd 520HR (ASTM Product Data Sheet)
Tensile Strength 83.0 MPa
12000 psi
at Break (NYP); ISO 527-1/-2
Quadrant EPP Semitron® ESd 520HR PAI, static dissipative, extruded (ISO Data)
Semitron ESd 520HR has an industry first combination of electrostatic dissipation (ESd), high strength and heat resistance. This new ESd material is ideal for making nests, sockets and contactors fo..
Tensile Strength 82.7 MPa
12000 psi
ASTM D638
Quantum Nylon 6/6
Information provided by Quantum Advanced Engineering Plastics
Tensile Strength 82.7 MPa
12000 psi
ASTM D638
Quantum Nylon 6/6 MoS2 Filled
Information provided by Quantum Advanced Engineering Plastics
Tensile Strength 83.0 MPa

@Temperature 23.0 °C
12000 psi

@Temperature 73.4 °F
DAM; ASTM D638
DuPont Performance Polymers Zytel® 45HSB NC010 Nylon 66  (Unverified Data**)
Zytel® 45HSB NC010 is a high viscosity, heat stabilized polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers
Tensile Strength 83.0 MPa
12000 psi
ISO 527
Lucite International Diakon® CLH952 Acrylic Polymer
Information provided by Lucite International
Tensile Strength 83.0 MPa
12000 psi
ISO 527
Lucite International Diakon® CLH952L Acrylic Polymer
Information provided by Lucite International
Tensile Strength 83.0 MPa
12000 psi
ISO 527
Lucite International Diakon® CLH952LX Acrylic Polymer
Information provided by Lucite International
Tensile Strength 83.0 MPa
12000 psi
ISO 527
Lucite International Diakon® CMG314V Acrylic Polymer
Information provided by Lucite International
Tensile Strength 83.0 MPa
12000 psi
ISO 527
Lucite International Diakon® CMG334V Acrylic Polymer
Information provided by Lucite International
Tensile Strength 82.7 MPa
12000 psi
ASTM D638
Haysite H320 Polyester Composite
A thermoset polyester composite that offers superior energy efficiency, temperature control, and durability for high temperature mold and platen thermal applications. A proven, cost effective produ..
Tensile Strength 82.7 MPa
12000 psi
ASTM D638
Haysite H330 Polyester Composite
A thermoset polyester composite that offers superior energy efficiency, temperature control, and durability for high temperature mold and platen thermal applications. A proven, cost effective produ..
Tensile Strength 82.7 MPa
12000 psi
ASTM D638
Teknor Apex Chemlon® 100 L Nylon 66, Unreinforced
Notes: Internally and externally lubricated; General Purpose; Double-lubricated for improved part ejection and machine feed Processing Method: Injection Molding Forms: PelletsInformation Provided by..
Tensile Strength 82.7 MPa
12000 psi
ASTM D638
Teknor Apex Chemlon® 223 Nylon 6, Unreinforced
Features: Nucleated for fast cyclingProcessing Method: Injection MoldingForms: Pellets Additive: Nucleating AgentInformation Provided by Teknor Apex
Tensile Strength >= 82.7 MPa
>= 12000 psi
Master Bond EP42HT-2ND-2Med Heat Resistant, Medical Grade Non-Drip Epoxy
Master Bond Polymer System EP42HT-2ND2MED (Black) is a room temperature curable two component epoxy adhesive and sealant featuring high temperature resistance along with outstanding chemical resista..
Tensile Strength >= 82.7 MPa
>= 12000 psi
Master Bond EP42HT-2FG Two Component Epoxy Adhesive for Food Applications
Master Bond Polymer System EP42HT-2FG is a room temperature setting, two component epoxy adhesive, sealant and coating specially formulated for food applications. It has been independently tested an..
Tensile Strength 83.0 MPa
12000 psi
ASTM D638
Lubrizol ESTALOC® 59300 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane
Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature ImpactUses: Injection MoldingAvailability: Americas, Europe, Middle East, Africa, India and AsiaInformation pro..
Tensile Strength 82.7 MPa
12000 psi
ASTM D638
Ensinger Tecapeek® XP-109 Compression Molded PEEK Compound, 30% Carbon Fiber with 15% PTFE
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in..
Tensile Strength 82.7 MPa
12000 psi
ASTM D638
Ensinger Tecapeek® XP-118 Compression Molded PEEK Compound, 20% Fiberglass with 5% PTFE
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in..
Tensile Strength 82.7 MPa
12000 psi
ASTM D638
Aaron Industries AAROPRENE® MFN 6001 Mineral Filled Nylon 6
AAROPRENE® GFN &G/MFN 6000 Series Reinforced CompoundsColor may be specified.
Tensile Strength 82.7 MPa
12000 psi
ASTM D638
Quadrant EPP Nylatron® MC® 907 Natural Nylon, Monocast® FDA Compliant, Unfilled Type 6 (ASTM Product Data Sheet)
Tensile Strength >= 82.7 MPa
>= 12000 psi
Master Bond EP42HT-2LO Low Outgassing, Heat Resistant Two Component Epoxy
Master Bond Polymer System EP42HT-2LO is a room temperature curable two component epoxy, adhesive, sealant, coating and casting material featuring high temperature resistance along with outstanding ..