Mechanical Properties Metric English Comments
Tensile Strength 60.0 - 90.0 MPa
8700 - 13100 psi
Compression; ISO 527
Raschig Group DECAL® 666/8/2B Phenolic
Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meets the allowe..
Tensile Strength 70.0 - 90.0 MPa
10200 - 13100 psi
Injection; ISO 527
Raschig Group DECAL® 666/8/2B Phenolic
Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meets the allowe..
Tensile Strength 70.0 - 90.0 MPa
10200 - 13100 psi
Injection and Compression; ISO 527
Raschig Group EPOXIDUR® 3581 S ZC EP Epoxy Molding Compound
Inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Very good sealing connection on ..
Tensile Strength 70.0 - 90.0 MPa
10200 - 13100 psi
Injection and Compression; ISO 527
Raschig Group EPOXIDUR® 3581 T-1 EP Epoxy, Molded, Glass Fiber Filler
Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Very ..
Tensile Strength 50.0 - 90.0 MPa
7250 - 13100 psi
Injection; ISO 527
Raschig Group MELOPAS® 2010 MF Melamine
Organically and inorganically filled Melamine molding compound. Excellent surface hardness, good mechanical strength, good electrical properties. This product meets the allowed upper limits for heav..
Tensile Strength 70.0 - 90.0 MPa
10200 - 13100 psi
Compression; ISO 527
Raschig Group DECAL® 152CL Phenolic
Glass-fiber and mineral reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meet..
Tensile Strength 70.0 - 90.0 MPa
10200 - 13100 psi
Compression; ISO 527
Raschig Group RESINOL® 400 EPF Phenolic
Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets ..