Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 150 MPa | 21800 psi | at Yield; ISO 527-1/-2 |
Quadrant EPP Duratron® PAI T4203 PAI, unfilled, extruded (ISO Data) Duratron T4203 PAI offers the best toughness and impact strength of all Duratron PAI grades. This extruded Duratron PAI grade is very popular for precision parts in high-tech equipment. In addition,.. |
|||
Tensile Strength | 150 MPa @Thickness 4.00 mm, Temperature 23.0 °C |
21800 psi @Thickness 0.157 in, Temperature 73.4 °F |
5.0 mm/min; ISO 527 |
PolyOne Bergamid™ B70 G45 BK Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Tensile Strength | 150 MPa | 21800 psi | at Yield; ISO 527-1/-2 |
Quadrant EPP Duratron® PAI T4503 PAI, unfilled, compression moulded (ISO Data) Compression moulded Duratron T4503 PAI is similar in composition to Duratron T4203 PAI, and is selected when larger shapes are required Very high maximum allowable service temperature in air (250°C.. |
|||
Tensile Strength | 150 MPa | 21800 psi | ASTM D638 |
PBI Performance Products Celazole® TF-60 V Glass Fiber Reinforced Melt Processable Polybenzimidazole Celazole® polybenzimidazole (PBI) resin is a unique and highly stable linear hetrocyclic polymer. PBI is characterized by high strength; excellent thermal stability, and broad chemical resistance. .. |
|||
Tensile Strength | 150 MPa | 21800 psi | ASTM D638 |
Kuraray Genestarâ„¢ GW1458HF Nylon, 45% Glass Filled Low Warpage, High Flow HB grade. Halogen free, following the standards that Br is less than 900ppm, Cl is less than 900ppm, and total of halogen amount (Br and Cl) is less than 1500ppm. |
|||
Tensile Strength | 150 MPa | 21800 psi | ASTM D638 |
Solvay Specialty Polymers Ryton® R-7-190NA Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-190NA glass fiber and mineral filled polyphenylene sulfide compound provides enhanced strength and low maintenance molding using conventional molding equipment.Features: Good Chemical .. |
|||
Tensile Strength | 150 MPa | 21800 psi | 5 mm/min; ISO 527-1 |
Sax Polymers SAXAMID 126F6T3 Nylon 6, 30% Glass Fiber and PTFE SAXAMID 126F6T3 is a polyamide 6 injection-molding-grade reinforced with 30% glass fibers and 15% PTFE. Because of its high strength and stiffness this grade is often used for stressed parts requiri.. |
|||
Tensile Strength | 150 MPa @Thickness >=1.50 mm |
21800 psi @Thickness >=0.0591 in |
24hr/23°C/50% RH; ISO 527; IEC/EN 60893-2 5.6 |
Elektro-Isola G-Etronax PM H Polyester, Glass Mat, Creme, Sheets Description: A reasonably-priced alternative to other high-temperature types. Low thermal conductivity. Applications: Used as, among other things, thermal insulation plates where high strength prope.. |
|||
Tensile Strength | >= 150 MPa | >= 21800 psi | IEC 1212-2 5.7 |
Hippe MF GC 201 Woven Glass Cloth Reinforced Melamine Resin - Sheet Used in mechanical and electrical applications. High mechanical strength. Arc and tracking resistant. Flame retardant. Information provided by Hippe. |
|||
Tensile Strength | 150 MPa | 21800 psi | dry; ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 GF30 FRV0 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grades, flammability class V0, reinforced with 30% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning.. |
|||
Tensile Strength | 150 MPa | 21800 psi | dry; ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 GF30 I Polyamide 6 - Glass Fiber Reinforced 30% Glass fiber reinforced, impact modified, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following mai.. |
|||
Tensile Strength | 150 MPa | 21800 psi | cond.; ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 GF50 Polyamide 6 - Glass Fiber Reinforced 50% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High.. |
|||
Tensile Strength | 150 MPa | 21800 psi | dry; ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 GF25 Polyamide 6 - Glass Fiber Reinforced 25% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High.. |
|||
Tensile Strength | 150 MPa | 21800 psi | ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 GF25 M Polyamide 6 - Improved Slip Properties Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Low wear and low friction grade, contains molybdenum disulfide, PTFE.Tarnamid.. |