Mechanical Properties Metric English Comments
Tensile Strength 131 MPa
19000 psi
ASTM D638
Quadrant EPP Ketron® CA30 LSG PEEK, Extruded 30% Carbon Fiber Reinforced Polyetherether Ketone (ASTM Product Data Sheet)
Tensile Strength 131 MPa
19000 psi
ASTM D638
Quadrant EPP Ketron® CA30 PEEK, Extruded 30% Carbon Fiber Reinforced Polyetherether Ketone (ASTM Product Data Sheet)
Tensile Strength 131 MPa
19000 psi
ASTM D638
Quantum Composites HTC-9590 55% Carbon Fiber Reinforced Bismaleimide SMC, High Temperature Composite
HTC-9590 (127-51-3) is a 12K Pan Based Carbon Fiber reinforced Bismaleimide (BMI) ESC (Engineered Structural Composite) molding compound. It exhibits outstanding elevated temperature characteristic..
Tensile Strength 131 MPa
19000 psi
Conditioned; ASTM D638
Solvay Specialty Polymers Amodel® AT-1116 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AT-1116 HS polyphthalamide (PPA) is a toughened, heat stabilized 16% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional stabi..
Tensile Strength 131 MPa
19000 psi
ASTM D638
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA), 65% GlassMineral (Dry)
Amodel® A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention..
Tensile Strength 131 MPa
19000 psi
ASTM D638
Solvay Specialty Polymers Amodel® AT-1116 HS Polyphthalamide (PPA), 16% Glass Fiber (Conditioned)
Amodel® AT-1116 HS polyphthalamide (PPA) is a toughened, heat stabilized 16% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional s..
Tensile Strength 131 MPa
19000 psi
ASTM D638
Solvay Specialty Polymers Ryton® R-7-120NA Polyphenylene Sulfide (PPS), GlassMineral Filled
Ryton® R-7-120NA and R-7-120BL glass fiber and mineral filled polyphenylene sulfide compounds provide good strength and low maintenance molding using conventional molding equipment.Features: Good..
Tensile Strength 131 MPa
19000 psi
ASTM D638
Solvay Specialty Polymers Ryton® R-7-121NA Polyphenylene Sulfide (PPS), GlassMineral Filled
Ryton® R-7-121NA and R-7-121BL glass fiber and mineral filled polyphenylene sulfide compounds provide good mechanical strength with good flow and low maintenance molding using conventional moldin..
Tensile Strength 131 MPa
19000 psi
5 mm/min; ISO 527-1
Sax Polymers SAXAMID 226F6RY01 Nylon 6.6, 30% Glass Fiber
SAXAMID 226F6RY01 is a polyamide 6.6 injection-molding-grade reinforced with 30% glass fibers. It has a halogen-free flame retardant.Information provided by SAX Polymers
Tensile Strength 131 MPa
19000 psi
ASTM D638
Solvay Specialty Polymers Ryton® XE5030BL Polyphenylene Sulfide Alloy (PPS Alloy), 30% Glass Fiber
Ryton® XE5030BL 30% glass fiber reinforced polyphenylene sulfide alloy compound provides high ductility and impact resistance along with good thermal stability.Features: Ductile; Good Thermal Sta..
Tensile Strength 131 MPa
19000 psi
Anderman Ceramics EA96 Sintered Alumina, 96%
High strength alumina (96%) available pink or white. Available in many shapes and sizes.Information provided by Anderman Ceramics.
Tensile Strength 131 MPa
19000 psi
Machine; ASTM D882
Arlon DiClad 522/527 PTFE/Woven Fiberglass Laminates
DiClad 522 and DiClad 527 use a higher fiberglass/PTFE ratio to provide mechanical properties approaching conventional substrates.Extremely Low Loss TangentExcellent Dimensional StabilityProduct Per..
Tensile Strength 131 MPa

@Temperature 22.8 °C
19000 psi

@Temperature 73.0 °F
ASTM D638
Quadrant EPP Duratron® U2100 OEI Extruded 10% Glass Reinforced Polyetherimide
Tensile Strength 131 MPa
19000 psi
ASTM D638
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA)  (Unverified Data**)