Mechanical Properties Metric English Comments
Tensile Strength 2.14 MPa
311 psi
ASTM D412
Northstar Polymers MPP-A50A High Performance Polyether
This high performance polyether system is one of a family of polymer systems developed by Northstar Polymers for specific demanding work environments. Urethane elastomers molded with this system ex..
Tensile Strength 2.14 MPa
311 psi
ASTM D412
Northstar Polymers MPG-A25A Room-Temperature Curable Liquid Castable Polyurethane
MPG-A25A is a room-temperature-cure liquid castable polyurethane system. This ether-base polyurethane system is used in applications such as mold-making, prototyping, production of cast parts, pott..