Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 40.0 MPa | 5800 psi | ISO 527 |
Premix Premi-Glas® 1266 (Injection Compression Molded) Glass Reinforced TMC Description: Premi-Glas® 1266 is a glass reinforced thermoset molding compound designed for automotive under the hood applications. Key features and benefits: Designed for Injection or Injection/Co.. |
|||
Tensile Strength | 40.0 MPa | 5800 psi | ASTM D638 |
Quadrant EPP TIVAR® 1000 UV Stabilized UHMW, Black (ASTM Product Data Sheet) |
|||
Tensile Strength | 40.0 MPa | 5800 psi | ASTM D638 |
Quadrant EPP TIVAR® ESD Electro Static Dissipative UHMW-PE (ASTM Product Data Sheet) Protects against electrical charge build-up Reduces noise Self-lubricating Corrosion-resistant No moisture absorption |
|||
Tensile Strength | 40.0 MPa | 5800 psi | ASTM D412 |
Northstar Polymers MSS-A85C Ester Base Polyurethane This high performance polyester system is one of a family of polymer systems developed by Northstar Polymers for demanding work environments. Urethane elastomers molded with this system exhibit hig.. |
|||
Tensile Strength | 40.0 - 60.0 MPa | 5800 - 8700 psi | Compression; ISO 527 |
Raschig Group 6551 DAIP Diallyl Phthalate (DAP), Cast, Mineral Filler Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi.. |
|||
Tensile Strength | 40.0 - 50.0 MPa | 5800 - 7250 psi | Compression; ISO 527 |
Raschig Group MELOPAS® 156 MF Melamine Glass fiber reinforced Melamine molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 200.. |
|||
Tensile Strength | 40.0 - 65.0 MPa | 5800 - 9430 psi | Compression; ISO 527 |
Raschig Group MELOPAS® 2010 MF Melamine Organically and inorganically filled Melamine molding compound. Excellent surface hardness, good mechanical strength, good electrical properties. This product meets the allowed upper limits for heav.. |
|||
Tensile Strength | 40.0 MPa | 5800 psi | ASTM D412 |
GRECO ISOTHANE 3065D Polyether TPU Resin ISOTHANE 3000 Series products are polyether based thermoplastic polyurethanes. They exhibit excellent hydrolytic resistance, fungus resistance, and low temperature performance properties. These prod.. |
|||
Tensile Strength | 40.0 - 55.0 MPa | 5800 - 7980 psi | DIN 53455 |
Isoflon ECTFE Fluoropolymer Fluoropolymer material specifications.Information provided by Isoflon. |
|||
Tensile Strength | 40.0 MPa | 5800 psi | ASTM D412 |
GRECO ISOTHANE 1160D Poly(adipate)ester TPUÂ Resin ISOTHANE 1100 series products are transparent grade, polyester poly(adipate)ester based thermoplastic polyurethanes. They exhibit good toughness, solvent resistance, easy processing, and high transp.. |
|||
Tensile Strength | 40.0 MPa | 5800 psi | ISO 527-1 |
Sax Polymers SAXLAC 310T Acrylonitrile Butadiene Styrene Saxalac 310T is an antistatic, high impact resistant ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% RH.Information provid.. |
|||
Tensile Strength | 40.0 MPa | 5800 psi | ISO 527-1 |
Sax Polymers SAXLAC 420HI Acrylonitrile Butadiene Styrene Saxalac 420HI is a flame retardant, very high flow ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% RH.Information provided.. |
|||
Tensile Strength | 40.0 MPa | 5800 psi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-7190 Polycaprolactone Based TPU Higher mechanical strength, good hydrolytic stability & chemical resistance, weather resistance, heat & fungus resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tensile Strength | 40.0 MPa | 5800 psi | ASTM D412 |
Lubrizol ESTANE® 58134 Ester Based Thermoplastic Polyurethane Features: Fast cycling, broad temperature performance, and durabilityUses: Injection Molding Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol. |
|||
Tensile Strength | 40.0 MPa | 5800 psi | ASTM D638 |
Lubrizol ESTALOC® 59104 Ester-Type, Reinforced Engineering Thermoplastic Features: Fast cycling, dimensional stability, durability, aesthetics, low temperature impactUses: Injection Molding Available in Americas and AsiaInformation provided by Lubrizol |
|||
Tensile Strength | 40.0 MPa | 5800 psi | ASTM D638 |
Ensinger Tecatron® XP-82 Compression Molded PPS Compound, Filled with 15% PTFE and 30% Carbon Fiber Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Tensile Strength | 40.0 MPa | 5800 psi | after storage in water at 80°C for 42 days; ISO 37 |
BASF Elastollan 685 AU TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tensile Strength | 40.0 MPa | 5800 psi | after storage in water at 80°C for 42 days; ISO 37 |
BASF Elastollan B 60 D TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup.. |
|||
Tensile Strength | 40.0 MPa | 5800 psi | after storage in water at 80°C for 42 days; ISO 37 |
BASF Elastollan B 64 D TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup.. |
|||
Tensile Strength | 40.0 MPa | 5800 psi | after storage in water at 80°C for 42 days; ISO 37 |
BASF Elastollan B 90 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup.. |
|||
Tensile Strength | 40.0 MPa | 5800 psi | ISO 37 |
BASF Elastollan SP 883 TPUR Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien.. |
|||
Tensile Strength | >= 40.0 MPa | >= 5800 psi | ISO 37 |
Austin Novel Materials Texalan® 485A Polyester-based TPU Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Tensile Strength | >= 40.0 MPa | >= 5800 psi | ISO 37 |
Austin Novel Materials Texalan® 590A Polyether-based TPU Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech |
|||
Tensile Strength | 40.0 MPa | 5800 psi | ASTM D638 |
Aaron Industries AAROPRENE® GFPP 2010 Glass Filled Polypropylene AAROPRENE® GFPP 2000 Series Glass Reinforced CompoundsMelt flow index may be specified. Color may be specified. |
|||
Tensile Strength | 40.0 MPa | 5800 psi | ISO 37 |
BASF Elastollan 664 DU TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tensile Strength | 40.0 MPa | 5800 psi | ISO 37 |
BASF Elastollan 880 AN TPUR Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien.. |
|||
Tensile Strength | 40.0 MPa | 5800 psi | 5 mm/min; ISO 527-1 |
Sax Polymers SAXAMID 236Q33 Nylon 6.6, Impact Modified SAXAMID 236Q33 is a impact-modified polyamide 6.6 injection-molding-grade with very good flow properties and outstanding toughness. Even at low temperatures this grade offers super-tough properties... |
|||
Tensile Strength | 40.0 MPa | 5800 psi | ISO 527-1 |
Sax Polymers SAXLAC 835T Acrylonitrile Butadiene Styrene Saxalac 835T is an antistatic, easy flowing ABS injection molding grade, characterized by high impact strength, high stiffness and good resistance to heat distortion.Mechanical property data tested .. |
|||
Tensile Strength | 40.0 MPa | 5800 psi | Weld; ASTM D638 |
Kuraray Genestar™ GN2450 Nylon, 45% Glass Filled High Strength V-0 Grade. Features a high strength and modulus. It is well suited for FPC sliders and IC sockets, as well as other components that require modulus and dimensional precision. |
|||
Tensile Strength | 40.0 - 50.0 MPa | 5800 - 7250 psi | ISO 527 |
Bulk Molding Compounds tetra-DUR F 4306 Bulk Molding Compound Mechanical high grade standard productTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion pr.. |