Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 40.0 - 65.0 MPa | 5800 - 9430 psi | Compression; ISO 527 |
Raschig Group MELOPAS® 2010 MF Melamine Organically and inorganically filled Melamine molding compound. Excellent surface hardness, good mechanical strength, good electrical properties. This product meets the allowed upper limits for heav.. |