Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 56.5 MPa | 8200 psi | ASTM D638 |
Techmer ES HiFill FR® PBT FR X Availability: North AmericaForms: PelletsAdditive: Mold ReleaseFeatures: Flame RetardantProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Tensile Strength | 56.5 MPa | 8200 psi | Machine; IPC TM-650 2.4.18.3 |
Arlon CLTE Microwave Printed Circuit Board Substrate CLTE is a ceramic powder-filled and woven micro fiberglass reinforced PTFE composite engineered to produce a stable, low water absorption laminate with a nominal Dielectric Constant of 2.98.Ceramic/.. |
|||
Tensile Strength | 56.5 MPa | 8200 psi | Machine; ASTM D882 |
Arlon CLTE-P Pre-Preg Bonding Layer Arlon's CLTE-P Prepreg Bonding Layer is a ceramic filled PTFE coated glass stock that is used as a bonding ply for CLTE, CLTE-X or CLTE-AT laminates. CLTE-P is a pre-preg material that consists of .. |
|||
Tensile Strength | 56.5 MPa | 8200 psi | ASTM D638 |
Techmer ES HiFill FR® PBT FR Availability: North AmericaForms: PelletsFeatures: Flame RetardantProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Tensile Strength | 56.5 - 70.3 MPa | 8200 - 10200 psi | |
Bulk Molding Compounds BMC T70 Automotive Grade Molding compound BMC T70 is a low profile automotive grade molding compound specifically formulated for the vacuum metallization process. These compounds have excellent physical properties as well as superior adhes.. |
|||
Tensile Strength | 56.5 MPa | 8200 psi | ASTM D638 |
Techmer ES HiFill FR® PBT FR-S Availability: North AmericaForms: PelletsFeatures: Flame Retardant and Non-BloomingProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |