Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 86.2 MPa @Temperature 22.8 °C |
12500 psi @Temperature 73.0 °F |
ASTM D638 |
Quadrant EPP KETRON® MD PEEK, A Metal-Detectable Polyetheretherketone |
|||
Tensile Strength | 86.2 MPa | 12500 psi | ASTM D638 |
Quadrant EPP Nylatron® GS Nylon, Extruded MoS2 Filled Type 66 (ASTM Product Data Sheet) |
|||
Tensile Strength | 86.2 MPa | 12500 psi | ASTM D638 |
Solvay Specialty Polymers Radel® R-7625 Polyphenylsulfone (PPSU) Radel® R-7625 polyphenylsulfone resin is a cost-effective solution for aircraft interior applications that offers improved UV resistance versus Radel® R-7535 and Radel® R-7558. The product .. |
|||
Tensile Strength | 86.2 MPa | 12500 psi | ASTM D638 |
Teknor Apex Beetle® 140 BH Nylon 66, Glass Bead Reinforced Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex |
|||
Tensile Strength | 86.2 MPa | 12500 psi | ASTM D638 |
Teknor Apex Chemlon® 100 Nylon 66, Unreinforced Features: Basic nylon 66 with internal lubrication. Widely used for automotive, electronic and appliance applications. Processing Method: Injection Molding Forms: Pellets Automotive Specifications: .. |
|||
Tensile Strength | 86.2 MPa | 12500 psi | ASTM D638 |
Aaron Industries AAROPRENE® MFN 6601 Mineral Filled Nylon 6/6 AAROPRENE® GFN & MFN 6600 Series Reinforced CompoundsColor may be specified. |
|||
Tensile Strength | 86.2 MPa | 12500 psi | ASTM D638 |
Teknor Apex Chemlon® 109-18 GH Nylon 66, 18% Glass Fiber Reinforced Notes: High-impact; Reinforced with 18% glass fibers; Highly toughened compound designed to improve practical toughness and ductility Features: Ductile; Good Impact Resistance; Good Toughness; Good .. |
|||
Tensile Strength | 86.2 MPa @Temperature 22.8 °C |
12500 psi @Temperature 73.0 °F |
ASTM D638 |
Quadrant EPP Duratron® PAI T7530, Compression Molded Carbon Fiber Reinforced Polyamide-Imide |
|||
Tensile Strength | 86.2 MPa @Temperature 22.8 °C |
12500 psi @Temperature 73.0 °F |
ASTM D638 |
Quadrant EPP Duratron® PAI T7530, Compression Molded Carbon Fiber Reinforced Polyamide-Imide |