Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 6.00 MPa | 870 psi | DIN 53504-S1 |
P & P Technology CB 70 Carbon Loaded Silicone Applications: Electrically conductive grades which when properly catalyzed can be considered for applications requiring conductivity such as EMI gaskets, conductive sheaths for ignition cable core,.. |
|||
Tensile Strength | 6.00 MPa | 870 psi | |
Momentive Performance Materials Siloprenâ„¢ Electro 242-1 Electrically Insulating Liquid Silicone Rubber This LSR elastomer is an electrically insulating, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Tensile Strength | 6.00 MPa | 870 psi | |
Momentive Performance Materials Siloprenâ„¢ FSL 7586/40 Fluorinated Liquid Silicone Rubber This LSR elastomer is a fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperature.. |
|||
Tensile Strength | 6.00 MPa | 870 psi | |
Momentive Performance Materials Siloprenâ„¢ FSL 7641 Fluorinated Liquid Silicone Rubber This LSR elastomer is a fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperature.. |
|||
Tensile Strength | 6.00 MPa | 870 psi | |
Momentive Performance Materials Siloprenâ„¢ LIM 9071E Liquid Silicone Rubber - Self-Bonding This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur.. |
|||
Tensile Strength | 6.00 MPa | 870 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 2020 Liquid Silicone Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Tensile Strength | 6.00 MPa | 870 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 2345/05 Electrically-Conductive Liquid Silicone Rubber This LSR elastomer is an electrically conductive, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Tensile Strength | 6.00 MPa | 870 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 2841 Liquid Silicone Rubber - Good Flex Life This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Tensile Strength | 6.00 MPa | 870 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 3286/50 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Tensile Strength | 6.00 MPa | 870 psi | |
Shandong Rike Chemical HELIâ„¢ HLC-135A PVC Impact Modifier-CPE Series Mechanism of Impact ModificationIt is found by research that the weak impact strength of PVC under lower temperature is mainly caused by stronger intermolecular force of PVC. Owing to stronger inte.. |
|||
Tensile Strength | 6.00 MPa | 870 psi | |
Shandong Rike Chemical HELIâ„¢ HLC-2235 PVC Impact Modifier-CPE Series Mechanism of Impact ModificationIt is found by research that the weak impact strength of PVC under lower temperature is mainly caused by stronger intermolecular force of PVC. Owing to stronger inte.. |
|||
Tensile Strength | 6.00 MPa | 870 psi | |
Shandong Rike Chemical HELIâ„¢ HLC-40B PVC Impact Modifier-CPE Series Mechanism of Impact ModificationIt is found by research that the weak impact strength of PVC under lower temperature is mainly caused by stronger intermolecular force of PVC. Owing to stronger inte.. |
|||
Tensile Strength | 6.00 MPa | 870 psi | ISO 527 |
Fainplast Compounds Hax™ HFC 0108 Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Bedding, designed to meet BS 6724Information provided by Fainplast Compounds |
|||
Tensile Strength | 6.00 MPa @Strain 20.0 % |
870 psi @Strain 20.0 % |
ISO 37 |
BASF Elastollan 695 AU TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tensile Strength | 6.00 MPa @Strain 300 % |
870 psi @Strain 300 % |
ISO 37 |
BASF Elastollan C 75 A HPM TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping c.. |
|||
Tensile Strength | 6.00 MPa @Strain 100 % |
870 psi @Strain 100 % |
ISO 37 |
BASF Elastollan C 88 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping c.. |
|||
Tensile Strength | 6.00 MPa | 870 psi | 100; ISO 37 |
BASF Elastollan SP 806 TPUR Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien.. |
|||
Tensile Strength | 6.00 MPa @Strain 100 % |
870 psi @Strain 100 % |
ISO 37 |
BASF Elastollan C 85 A HPM TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping c.. |
|||
Tensile Strength | 6.00 MPa | 870 psi | |
Momentive Performance Materials Silopren™ LSR 3386/30 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Tensile Strength | 6.00 MPa | 870 psi | |
Momentive Performance Materials XE23-703U Heat Cured Rubber - Electro Conductive Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |