Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 60.0 MPa | 8700 psi | ASTM D638 |
Premix Premi-Glas® 1200-25 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200-25 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Tensile Strength | 60.0 MPa | 8700 psi | ASTM D638 |
Premix Premi-Glas® 1200H-25 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200H-25 is a fiberglass reinforced thermoset sheet molding compound for general purpose and HVAC applications requiring thermal stability and stiffness.Key features and benefits are:Go.. |
|||
Tensile Strength | 60.0 MPa | 8700 psi | ASTM D638 |
Premix Premi-Glas® 1240-25 Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 1240-25 is a fiberglass reinforced thermoset Thick Molding Compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Tensile Strength | 60.0 MPa | 8700 psi | at Yield; ISO 527-1/-2 |
Quadrant EPP Symalit® 1000 PVDF unfilled, extruded (ISO Data) Symalit 1000 PVDF is a highly crystalline unreinforced fluoropolymer combining good mechanical, thermal and electrical properties with excellent chemical resistance. It also shows good resistance to.. |
|||
Tensile Strength | 60.0 - 90.0 MPa | 8700 - 13100 psi | Compression; ISO 527 |
Raschig Group DECAL® 666/8/2B Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meets the allowe.. |
|||
Tensile Strength | 60.0 - 85.0 MPa | 8700 - 12300 psi | Injection; ISO 527 |
Raschig Group MELOPAS® 6605 MP Melamine Cellulose reinforced Melamine molding compound. Very good electrical properties, excellent surface hardness, good mechanical strength and heat resistance, good wear and UV-stability, good gliding be.. |
|||
Tensile Strength | 60.0 MPa | 8700 psi | Weld; ASTM D638 |
Kuraray Genestarâ„¢ GT2330 Nylon, 33% Glass Filled Toughness V-0 Grade. It is well suited for components requiring a high strength in pin fitting process, due to high ductility properties. |
|||
Tensile Strength | 60.0 MPa | 8700 psi | GB/T 1040.2-2006 |
Sichuan Deyang Haton® hFR70 PPS / AR Polyphenylene Sulfide Injection molding, themal conductionInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Tensile Strength | 60.0 MPa | 8700 psi | GB/T 1040.2-2006 |
Sichuan Deyang Haton® hFR81 Polyphenylene Sulfide Injection molding, reinforcedInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Tensile Strength | 60.0 MPa | 8700 psi | ASTM D638 |
Techmer ES Luriblend® TPX-PA6/6-95001 Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Tensile Strength | 60.0 MPa | 8700 psi | ASTM D638 |
Techmer ES HiFill® ABS GF20 FR 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Tensile Strength | 60.0 MPa | 8700 psi | ASTM D412 |
Lubrizol ESTANE® ETE50DT3 Ester Based Thermoplastic Polyurethane Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, high transparency, UV stableUses: Extrusion: Hose and Tube, Profile, Cable Jacket; Injection.. |
|||
Tensile Strength | 60.0 MPa | 8700 psi | dry; ISO 527 |
Ter Hell Plastic Terez® PA 6.6 7750 T Polyamide 66 Description: Dry impact unfilled Polyamide 6.6, good flowability and demolding properties.Application: Molding parts of different kinds, high impact properties.Information provided by Ter Hell Plas.. |
|||
Tensile Strength | 60.0 MPa | 8700 psi | dry; ISO 527 |
Ter Hell Plastic Terez® PBT 6750 T Polybutylene Terephthalate, Impact Modified Description: Impact modified PBT.Application: For impact stressed, injection molding parts.Information provided by Ter Hell Plastic GMBH. |
|||
Tensile Strength | 60.0 MPa | 8700 psi | dry; ISO 527 |
Ter Hell Plastic Terez® PC X 9005 GF 5 Polycarbonate, 5% Glass Fiber Description: Polycarbonate, medium flowability, 5% glass fiber reinforced.Application: For injection molded parts with increased demand of stiffness.Information provided by Ter Hell Plastic GMBH. |
|||
Tensile Strength | >= 60.0 MPa | >= 8700 psi | IEC 1212-2 5.7 |
Hippe MF CC 201 Woven Cotton Cloth Reinforced Melamine Resin - Sheet Used in mechanical and electrical applications (coarse weave: >130 g/m2, =30 threads/cm). Arc and tracking resistant.Information provided by Hippe. |
|||
Tensile Strength | >= 60.0 MPa | >= 8700 psi | IEC 1212-2 5.7 |
Hippe PF CP 205 Cellulose Paper Reinforced Phenolic Resin - Sheet Used in electrical and electronic applications. Good stability of electrical properties under high humidity. Also available in cold or hot-punching versions. Flame retardant.Information provided .. |
|||
Tensile Strength | >= 60.0 MPa | >= 8700 psi | IEC 1212-2 5.7 |
Hippe PF WV 201 Wood veneer Reinforced Phenolic Resin - Sheet Cross plied. Used in mechanical applications. Good mechanical properties.Information provided by Hippe. |
|||
Tensile Strength | >= 60.0 MPa | >= 8700 psi | IEC 1212-2 5.7 |
Hippe PF WV 202 Wood veneer Reinforced Phenolic Resin - Sheet Cross plied. Used in mechanical and electrical applications. Good electrical properties under normal humidity.Information provided by Hippe. |
|||
Tensile Strength | 60.0 MPa | 8700 psi | DIN 53 455 |
Hippe PMMA Components made of PMMA are brilliantly transparent. Outstanding aging stability and weathering resistance. Good surface hardness. Abrasion-resistant. Physiologically safe. High strength. Easi.. |
|||
Tensile Strength | 60.0 MPa | 8700 psi | cond.; DIN 53 455 |
Hippe PA 6 G Thick-wall pre-forms, heavy semi-finished products. Transfusion of inserts (rolls, cores) and all types of large preforms.Information provided by Hippe. |
|||
Tensile Strength | >= 60.0 MPa | >= 8700 psi | IEC 1212-2 5.7 |
Hippe PF CC 202 Woven Cotton Cloth Reinforced Phenolic Resin - Sheet Used in mechanical and electrical applications (coarse weave: >130 g/m2, =30 threads/cm).Information provided by Hippe. |
|||
Tensile Strength | 60.0 MPa | 8700 psi | 50 mm/min; ISO 37 |
BASF Elastollan R 2001 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Tensile Strength | 60.0 MPa @Strain 8.00 %, Temperature 40.0 °C |
8700 psi @Strain 8.00 %, Temperature 104 °F |
50 mm/min; ISO 527-2 |
BASF Elastollan R 3000 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Tensile Strength | 60.0 - 79.3 MPa | 8700 - 11500 psi | ASTM D638 |
Cast Nylons Nycast® CP Caprolactam/Laurinlactum Copolymer Cast Nylon Highly resilient, with higher tensile elongation and impact strength than standard grades, NYCAST® CP is used applications requiring an extra degree of toughness. A copolymer of caprolactam and lau.. |
|||
Tensile Strength | 60.0 MPa | 8700 psi | ASTM D638 |
Aaron Industries AAROPRENE® AEPC 5000-4 Engineered Polycarbonate Resin Melt flow index may be specified. |