Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 900 - 1100 MPa | 131000 - 160000 psi | Longitudinal |
Goodfellow Carbon/Vinyl Ester Rod Carbon Fiber - Vinyl ester MatrixInformation provided by Goodfellow. |
|||
Compressive Strength | 900 - 1100 MPa | 131000 - 160000 psi | Longitudinal |
Goodfellow Carbon/Vinyl Ester Tube Carbon Fiber - Vinyl ester MatrixInformation provided by Goodfellow. |